MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Plenco 5482 Phenolic, Granular, Transfer Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Woodflour Filled

Material Notes: PLENCO 05482 is an organic reinforced phenolic molding compound formulated with graphite to improve the abrasion resistance. 05482 is available in black and brown. 05482 is not recommended for electrical insulating applications.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.650 g/cc0.0235 lb/in³ASTM D1895
Density 1.43 g/cc0.0517 lb/in³ASTM D792
Water Absorption 0.247 %0.247 %ASTM D570
Linear Mold Shrinkage 0.0061 cm/cm0.0061 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 8989ASTM D785
Tensile Strength, Ultimate 55.0 MPa7980 psiASTM D638
Elongation at Break 0.41 %0.41 %ASTM D638
Tensile Modulus 8.70 GPa1260 ksiASTM D638
Flexural Strength 86.0 MPa12500 psiASTM D790
Flexural Modulus 8.00 GPa1160 ksiASTM D790
Compressive Strength 215 MPa31200 psiASTM D695
Izod Impact, Notched 0.180 J/cm0.337 ft-lb/inASTM D256
Charpy Impact, Notched 0.194 J/cm²0.923 ft-lb/in²ASTM D256
Impact 9696J/m Drop Ball Impact; PLENCO
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 201 °C394 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 186 °C367 °FASTM D648
Oxygen Index 28.5 %28.5 %ASTM D2863
Shrinkage 0.25 %0.25 %72 hr, 120ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLEM04 / 50680

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.