MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

BASF Petra® 7030 GY6128 30% Glass Filled PET
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 30% Glass Reinforced

Material Notes: Petra 7030 GY6128 is a grey pigmented, high flow 30% glass fiber reinforced injection molding compound based on post-consumer and post-industrial recycled polyethylene terephthalate feedstock. It offers strength, stiffness, and rigidity combined with excellent dimensional stability, creep resistance and high temperature performance. It's improved flow results in excellent urface aesthetics which can eliminate the need for painting parts.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.55 g/cc0.0560 lb/in³ISO 1183
Viscosity Measurement 0.550.55Inherent Viscosity
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inASTM Data; MD
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 118118ASTM Test
Tensile Strength at Break 150 MPa21800 psi0.2 in/min; ASTM Test
Tensile Strength, Ultimate 150 MPa21800 psi5mm/min; ISO 527
Elongation at Break 3.0 %3.0 %5mm/min; ISO 527
 3.0 %3.0 %0.2 in/min; ASTM Test
Flexural Strength 240 MPa34800 psiASTM Test
Flexural Modulus 8.83 GPa1280 ksiISO Data
 9.09 GPa1320 ksiASTM Test
Izod Impact, Notched 1.00 J/cm
@Thickness 3.17 mm
1.87 ft-lb/in
@Thickness 0.125 in
ASTM Test
Izod Impact, Notched (ISO) 9.50 kJ/m²4.52 ft-lb/in²ISO Test
 
Thermal PropertiesMetricEnglishComments
CTE, linear 23.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
12.8 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM Test
Melting Point 245 °C473 °F10 K/min
 245 °C473 °FASTM Test
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 275 °C527 °FInjection molding
Mold Temperature 115 °C239 °FInjection molding
 
Descriptive Properties
ColorGY6128
Commercial StatusActive America
FormPellets
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
7030 Aluminum Composition Spec
BASF Petra® 7010 BK 5830 15% Glass Filled PET
BASF Petra® 130 30% Glass Filled PET
Cotronics Resbond™ 7030 High Temperature Ceramic Adhesive, High Strength
BASF Petra® 130 FR 30% Glass Filled PET

PBASF9024 / 84788

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.