MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ATI Allegheny Ludlum Grade 12 Titanium (UNS R53400)
Categories: Metal; Nonferrous Metal; Titanium Alloy; Unalloyed/Modified Titanium

Material Notes: Uses: heat exchangers, industrial components, tubing, CPI equipment.

Mechanical property data below is typical of annealed samples at room temperature.

Information provided by Allegheny Ludlum.

Key Words: ASTM B-265; ASME SB-265; DIN 3.7105
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.52 g/cc0.163 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 180180
Tensile Strength, Ultimate 620 MPa89900 psi
Tensile Strength, Yield 450 MPa
@Strain 0.2 %
65300 psi
@Strain 0.2 %
Elongation at Break 22 %22 %
 
Component Elements PropertiesMetricEnglishComments
Molybdenum, Mo 0.30 %0.30 %
Nickel, Ni 0.80 %0.80 %
Titanium, Ti 98.9 %98.9 %as balance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Grade 12, Annealed
Overview of materials for Unalloyed/Modified Titanium
Kobe Steel KSG12 Titanium alloy with low alloying elements, ASTM Gr. 12, Annealed
Industeel CLC 17.12.2 Ti Titanium Stabilized 18Cr-11Ni-2Mo Austenitic Stainless Steel
Goodfellow Titanium 88/Aluminum 12 Alloy

NLTIT12 / 18060

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.