MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Celanese Hostaform® S 9244 XAP2™ LS POM, Impact Modified
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Impact Modified

Material Notes: POM copolymer, modified

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc0.0455 lb/in³ISO 1183
Water Absorption at Saturation 1.2 %1.2 %ISO 62
Linear Mold Shrinkage, Flow 0.017 cm/cm0.017 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.016 cm/cm0.016 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 33.0 MPa4790 psi50mm/min; ISO 527-2/1A
Elongation at Break >= 50 %>= 50 %ISO 527-2/1A
Elongation at Yield 7.0 %7.0 %50mm/min; ISO 527-2/1A
Tensile Modulus 1.45 GPa210 ksi1mm/min; ISO 527-2/1A
Flexural Modulus 1.45 GPa210 ksiISO 178
Charpy Impact Unnotched NBNBISO 179/1eU
 20.0 J/cm²
@Temperature -30.0 °C
95.2 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.80 J/cm²8.57 ft-lb/in²ISO 179/1eA
 1.20 J/cm²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
Tensile Creep Modulus, 1 hour 1200 MPa174000 psiISO 899-1
Tensile Creep Modulus, 1000 hours 650 MPa94300 psiISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant  3.6
@Frequency 1e+6 Hz
3.6
@Frequency 1e+6 Hz
IEC 60250
 3.6
@Frequency 100 Hz
3.6
@Frequency 100 Hz
IEC 60250
Dissipation Factor  0.0040
@Frequency 100 Hz
0.0040
@Frequency 100 Hz
IEC 60250
 0.0060
@Frequency 1e+6 Hz
0.0060
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 130 µm/m-°C72.2 µin/in-°FISO 11359-2
Melting Point 166 °C331 °FISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C154 °FISO 75-1, -2
Vicat Softening Point 115 °C239 °FB50 (50°C/h 50N); ISO 306
 
Descriptive Properties
Injection moldingYes
Melt volume rate (MVR), cm³/10min1.4
MVR test load, kg2.16
MVR test temperature, °C190
Processing conditions acc. ISO9988-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHCS400 / 123815

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.