MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Lehmann & Voss LUVOCOM® 20-7094 Polyphthalamide with carbon fiber and PTFE
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), Carbon Fiber + PTFE Filled

Material Notes: Properties/attributes include: Very strong and stiff parts; low coefficient of thermal expansion. Low influence from moisture and temperature to measures and electrical properties, compared with PA66 Suitable for metal inserts. Improved friction and wear behavior. Emergency (dry) running property.

Automotive industry, textile- and office machinery, apparatus- and precision engineering. Typical uses include: Bearings, sleeves, sliding elements, control disks, gear wheels, duty parts in switches.

Processing: During processing the moisture level should not exceed 0.05%, otherwise molecular degradation and surface defects (e.g. smearing) may occur. Processing temperatures above 340°C may very rapidly cause thermal damage and should therefore be avoided. The processing notes provided merely represent a recommendation for general use. Due to the large variety of machines, geometries and volumes of parts, etc., it may be necessary to employ different settings according to the specific application. High-temperature polymers place increased demands on the tool steels employed.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.44 g/cc1.44 g/ccISO 1183
Moisture Absorption <= 0.300 %
@Temperature 23.0 °C,
Time 86400 sec
<= 0.300 %
@Temperature 73.4 °F,
Time 24.0 hour
Linear Mold Shrinkage 0.00050 - 0.0030 cm/cm0.00050 - 0.0030 in/inDIN 16901
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 270 MPa39200 psiISO 527-2
Elongation at Break 1.5 %1.5 %ISO 527-2
Modulus of Elasticity 25.0 GPa3630 ksiISO 527-2
Flexural Strength 385 MPa55800 psiISO 178
Flexural Modulus 21.0 GPa3050 ksiISO 178
Flexural Strain at Break 1.9 %1.9 %Flexural Elongation @ Fmax; ISO 178
Charpy Impact Unnotched 5.50 J/cm²
@Temperature 23.0 °C
26.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eU
Charpy Impact, Notched 0.800 J/cm²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity <= 1000 ohm-cm<= 1000 ohm-cmIEC 60167
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 165 °C329 °FContinuous; UL 746B
 195 °C383 °FShort Term
Deflection Temperature at 1.8 MPa (264 psi) 275 °C527 °FISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 320 - 330 °C608 - 626 °F
Zone 1 320 - 340 °C608 - 644 °F
Zone 2 320 - 345 °C608 - 653 °F
Zone 3 325 - 350 °C617 - 662 °F
Melt Temperature 330 °C626 °F
Mold Temperature 135 - 160 °C275 - 320 °F
Drying Temperature  80.0 °C
@Time >=57600 sec
176 °F
@Time >=16.0 hour
Dehumidifying dryer
 105 °C
@Time 14400 - 18000 sec
221 °F
@Time 4.00 - 5.00 hour
Vacuum Dryer
Moisture Content <= 0.050 %<= 0.050 %
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyphthalamide (PPA)
Overview of materials for Polyphthalamide (PPA), Glass/PTFE
Overview of materials for Polyetheretherketone, Glass Fiber Filled
LATI Laramid G/60 PPA, 60% Glass Fiber Reinforced
Evonik Trogamid® T-GF35 35% Glass Reinforced Amorphous Nylon

PLUU8911 / 193870

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.