MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Trelleborg Emerson & Cuming Eccobond® 286 Two-Component General Purpose Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy, Thermally Conductive

Material Notes: Emerson & Cuming 286 Eccobond® Two-Component General Purpose Epoxy Adhesive
Filled, general purpose, thermally conductive, epoxy adhesive. Room temperature cure. Convenient mix ratio. Recommended for a wide variety of maintenance and production applications. Ideal for use in piping applications involving metal and plastic pipe. Mix ratio of 100:100 (volume). Bonding Type: Epoxy

The Eccobond® product line is now a part of Henkel; this specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.71 g/cc0.0618 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength 15.2 MPa2200 psi
 
Processing PropertiesMetricEnglishComments
Cure Time  120 min
@Temperature 65.0 °C
2.00 hour
@Temperature 149 °F
 240 min
@Temperature 45.0 °C
4.00 hour
@Temperature 113 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
 
Descriptive Properties
ColorWhite
ViscosityThixotropic Paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Abatron AboCast 8-7/Abocure 8-7 Epoxy
Corning Macor® Machinable Glass Ceramic
DuPont™ 7723 Silver Conductor
ATI Allvac® Nickelvac® A-286 Specialty Steel, Heat Treatment: 982°C (1800°F) + Age
Armstrong A-34 Epoxy Adhesive

PEMERS46 / 35738

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.