Data provided by Allvac. Applications: Airframe skin, heat exchangers, cryogenic vessels, components for CPI equipment, condenser tubing, exhaust pipe shrouds. |
UNS R50550; AMS 4900; MIL-T-9046, -81556. ASTM F 67, Titanium Grade 3; ASTM B 265, 337, 338, 348.; Allvac, an Allegheny Teledyne Company |