ForTii® is a high temperature polyamide for applications in the electronics, lighting, automotive, white goods, industrial and aerospace industries. ForTii® XS81B has excellent impact resistance and high stiffness. It's good processing ability allow for high cosmetic requirements and good bonding in various painting process. XS81B is very suitable for mobile phone middle frame applications due to low warpage and excellent performance in tumbling tests. Features: 50% glass reinforced. Processing: Injection molding. Former DSM Engineering Plastics product line is now with Envalior. |