MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Resinoid 2020 Phenolic Molding, Fabric Reinforced
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Fabric Filled

Material Notes: Data provided by the manufacturer.

The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ASTM D792A
Water Absorption 0.50 %0.50 %24 hours R.T. ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inPositive Mold; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 48.0 MPa6960 psiASTM D651
Compressive Strength 159 MPa23100 psiASTM D695
Izod Impact, Notched 1.103 J/cm2.066 ft-lb/inASTM D256A
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 8.70 kV/mm221 kV/inShort Time; Dry; ASTM D149
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Mold Temperature 155 - 180 °C311 - 356 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zytel® 80G33HS1L NC010 PA66-IGF33
A. Schulman BMC T44-15613 High Strength Mineral Filled Molding Compound
Sumitomo Bakelite RX® 643 Phenolic Resole Compound
Sumitomo Bakelite North America RX® 640 Fiberglass Reinforced Phenolic Resole
Sumitomo Bakelite GF 8202 L24 Phenolic Novolac Molding Compound

PPHR0O / 56247

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.