MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

LATI Laticonther 57 CPG/550 PPA, Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 50% Glass Fiber Reinforced

Material Notes: High thermal conductivity product based on Semi-aromatic polyamide (PPA). Special filler. Glass fibers.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.99 g/cc0.0719 lb/in³
Linear Mold Shrinkage, Flow 0.0030 - 0.0045 cm/cm0.0030 - 0.0045 in/in
Linear Mold Shrinkage, Transverse 0.0050 - 0.0065 cm/cm0.0050 - 0.0065 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 70.0 MPa10200 psi
Elongation at Break 0.60 %0.60 %
Tensile Modulus 11.0 GPa1600 ksi
Charpy Impact Unnotched 1.00 J/cm²4.76 ft-lb/in²
Charpy Impact, Notched 0.200 J/cm²0.952 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+12 ohm1.00e+12 ohm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.20 W/m-K8.33 BTU-in/hr-ft²-°FLongitudinal
Deflection Temperature at 0.46 MPa (66 psi) 120 °C248 °F
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °F
Vicat Softening Point 100 °C
@Load 5.00 kg
212 °F
@Load 11.0 lb
 
Processing PropertiesMetricEnglishComments
Melt Temperature 310 - 330 °C590 - 626 °F
Mold Temperature 140 - 160 °C284 - 320 °F
Drying Temperature 120 - 130 °C
@Time 10800 sec
248 - 266 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® T1 GF 50 9 (3257) PPA Conditioned, 50% Glass Filled
PlastiComp Complet® LGF50-PPA Polyphthalamide, 50% Long Glass Fiber Reinforced
Syensqo (Solvay Specialty Polymers) Amodel® AF-1550 V0 Polyphthalamide (PPA) Resin, 50% Glass/Mineral Reinforced, at 50% RH
Akro-Plastic Akromid® T1 GF 50 (3101) PPA Conditioned, 50% Glass Filled
A. Schulman BMC 8005 Polyester Molding Compound

PLATH9797 / 177493

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.