MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Arkema Kynar® ADX FLEX 281 G PVDF
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes:

Information provided by Arkema Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.72 g/cc1.72 g/ccCoating; ISO 1183
Density 1.77 g/cc0.0639 lb/in³ISO 1183
Water Absorption <= 0.10 %
@Time 86400 sec
<= 0.10 %
@Time 24.0 hour
ISO 62-1
Particle Size 88.5 µm88.5 µmMedian; ISO 13320
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7575ISO 868
Impact Test 2.50 J1.84 ft-lbImpact Resistance; ASTM G14
Taber Abrasion, mg/1000 Cycles 33.533.5Wheel CS 17, load 1 kg; ISO 9352
 
Thermal PropertiesMetricEnglishComments
Melting Point 152 °C306 °FISO 1218
 158 °C316 °FISO 11357-3
Flammability, UL94 V-0V-0on coated panel
Oxygen Index 43 %43 %ASTM D2863
 
Descriptive Properties
Approximate RAL number6009
ColorGreen
Covering Efficiency (kg/m²)0.8
Covering Efficiency, Thickness (µm)500
Form as DeliveredPowder
Grade Package Weight - Bags (lb/bag)55
Heat StabilizedYes
Light StabilizedYes
Moisture SensitiveNo
Persoz Hardness207ISO 1522
Salt Spray TestGood adhesion after 2000 hoursISO 9227 (surface preparation per ARKEMA)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PARKF746b / 291176

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.