MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Syensqo (Solvay Specialty Polymers) AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Polyketone; Polyaryletherketone (PAEK), Glass Fiber Filled

Material Notes: AvaSpire® AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical strength and stiffness than unfilled AV-650 resin. This material can be repeatedly exposed to harsh chemicals and prolonged steam sterilization cycles without any significant loss of properties. Potential applications for this resin include orthopedic and dental instruments, surgical power tool battery housings and other devices and components requiring a combination of high temperature performance and high environmental resistance. AvaSpire® AV-650 GF30 can be easily processed by typical injection molding and extrusion methods using standard equipment.

Features: Fatigue Resistant; Flame Retardant; Good Chemical Resistance; Good Dimensional Stability; High Heat Resistance; High Stiffness; High Strength

Uses: Medical/Healthcare Applications; Oil/Gas Applications; Power/Other Tools

Additional Properties: Water Absorption - ASTM D570 0.40 %

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.55 g/cc0.0560 lb/in³ASTM D792
Filler Content 30 %30 %Glass Fiber
Water Absorption 0.20 %
@Time 86400 sec
0.20 %
@Time 24.0 hour
ISO 62
Viscosity 410000 cP
@Shear Rate 1000 1/s,
Temperature 400 °C
410000 cP
@Shear Rate 1000 1/s,
Temperature 752 °F
Melt Viscosity; ASTM D3835
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
@Thickness 3.18 mm
0.0010 - 0.0030 in/in
@Thickness 0.125 in
Linear Mold Shrinkage, Transverse 0.0080 - 0.010 cm/cm
@Thickness 3.18 mm
0.0080 - 0.010 in/in
@Thickness 0.125 in
ASTM D955
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 400 °C
15 g/10 min
@Load 4.76 lb,
Temperature 752 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 100100ASTM D785
Tensile Strength 142 MPa20600 psiASTM D638
Tensile Strength, Yield 165 MPa23900 psi5 mm/min, Type 1A; ISO 527-2
Elongation at Break 2.6 %2.6 %Type 1A, 5 mm/min; ISO 527-2
 2.6 %2.6 %5 mm/min; ASTM D638
Tensile Modulus 10.1 GPa1460 ksiASTM D638
 10.5 GPa1520 ksiISO 527-2
Flexural Strength 221 MPa32100 psiASTM D790
 240 MPa34800 psiISO 178
Flexural Modulus 9.00 GPa1310 ksiASTM D790
 9.80 GPa1420 ksiISO 178
Compressive Strength 163 MPa23600 psiASTM D695
Shear Strength 80.8 MPa11700 psiASTM D732
Izod Impact, Notched 0.960 J/cm1.80 ft-lb/inASTM D256
Izod Impact, Unnotched 9.60 J/cm18.0 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 13.0 kJ/m²6.19 ft-lb/in²ISO 180
Izod Impact, Unnotched (ISO) 69.0 kJ/m²32.8 ft-lb/in²ISO 180
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.6
@Frequency 1e+6 Hz
3.6
@Frequency 1e+6 Hz
ASTM D150
 3.65
@Frequency 60 Hz
3.65
@Frequency 60 Hz
ASTM D150
 3.66
@Frequency 1000 Hz
3.66
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 14.0 kV/mm
@Thickness 3.18 mm
356 kV/in
@Thickness 0.125 in
ASTM D149
Dissipation Factor  0.0020
@Frequency 60 Hz
0.0020
@Frequency 60 Hz
ASTM D150
 0.0050
@Frequency 1e+6 Hz
0.0050
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 19.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
10.6 µin/in-°F
@Temperature -58.0 - 122 °F
Specific Heat Capacity  1.29 J/g-°C
@Temperature 50.0 °C
0.308 BTU/lb-°F
@Temperature 122 °F
ASTM C351
 1.67 J/g-°C
@Temperature 200 °C
0.399 BTU/lb-°F
@Temperature 392 °F
ASTM C351
Thermal Conductivity 0.290 W/m-K2.01 BTU-in/hr-ft²-°FASTM C177
Melting Point 340 °C644 °FASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 209 °C
@Thickness 3.20 mm
408 °F
@Thickness 0.126 in
Annealed; ASTM D648
Glass Transition Temp, Tg 158 °C316 °FDSC
Flammability, UL94 V-0
@Thickness 0.800 - 1.60 mm
V-0
@Thickness 0.0315 - 0.0630 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 365 °C689 °F
Middle Barrel Temperature 370 °C698 °F
Front Barrel Temperature 375 °C707 °F
Nozzle Temperature 380 °C716 °F
Melt Temperature 365 - 390 °C689 - 734 °F
Mold Temperature 150 - 180 °C302 - 356 °F
Drying Temperature 150 °C
@Time 14400 sec
302 °F
@Time 4.00 hour
 
Descriptive Properties
Agency RatingsFAA FAR 25.853a
AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 Latin America
 North America
ColorBeige
FormPellets
Injection RateFast
Processing TechniqueInjection Molding; Machining; Profile Extrusion
Screw Compression Ratio2.0:1.0 to 3.0:1.0

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 3805 Polyaryletherketone (PAEK), Glass Fiber 30%
RTP Company RTP 3803 Polyaryletherketone (PAEK), Glass Fiber 20%
Akro-Plastic Akrotek® PEEK GF 30 natural (5047) PEEK, Dry, 30% Glass Filled

PSOL8Y7015 / 176746

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.