MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Hippe PF CP 203 Cellulose Paper Reinforced Phenolic Resin - Sheet
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Cellulose Filled

Material Notes: Used in mechanical and electrical applications. Good electrical properties under normal humidity. Also available in hot-punching versions.

Information provided by Hippe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 - 1.40 g/cc1.30 - 1.40 g/ccIEC 1212-2 8.1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 100 MPa>= 14500 psiIEC 1212-2 5.7
Flexural Strength >= 120 MPa>= 17400 psiPerpendicular to laminations; IEC 1212-2 5.1
Flexural Modulus >= 7.00 GPa>= 1020 ksiIEC 1212-2 5.2
Compressive Strength >= 250 MPa>= 36300 psiPerpendicular to laminations; IEC 1212-2 5.3
Shear Strength >= 10.0 MPa>= 1450 psiParallel to laminations; IEC 1212-2 5.6
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance >= 5.00e+7 ohm>= 5.00e+7 ohmAfter immersion in water; IEC 1212-2 6.3
Dielectric Constant <= 5.5
@Frequency 1e+6 Hz
<= 5.5
@Frequency 1e+6 Hz
IEC 1212-2 6.2
Dielectric Breakdown >= 20000 V
@Temperature 90.0 °C
>= 20000 V
@Temperature 194 °F
In oil, parallel to laminations; IEC 1212-2 6.2
Dissipation Factor <= 0.050
@Frequency 1e+6 Hz
<= 0.050
@Frequency 1e+6 Hz
IEC 1212-2 6.2
Comparative Tracking Index >= 100 V>= 100 VIEC 1212-2 6.4
 
Descriptive Properties
Thermal Endurance105 T.I.IEC 1212-2 7.1
Water Absorption< 320 mgIEC 1212-2 8.2; Test piece 50 x 50 x 10 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 6063-T5
LE Phenolic Laminate
Hippe PF CP 201 Cellulose Paper Reinforced Phenolic Resin - Sheet

PHIPPE918 / 121922

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.