MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

BASF Elastollan® R 3000 20% Glass Filled TPUR
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expansion comparable with steel and aluminum, low mold shrinkage and ease of painting.

Typical Applications: Automotive body and rocker panels, underbody sealants, technical moldings e.g. plugs and ski tips.

Note: Quoted results are from measurements on injection molded test platens, post tempered for 20 hours at 100°C

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³ISO 1183-1-A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7373ISO 686
Tensile Strength 80.0 MPa11600 psi50 mm/min; ISO 37
 30.0 MPa
@Strain 2 %,
Temperature 60.0 °C
4350 psi
@Strain 2 %,
Temperature 140 °F
50 mm/min; ISO 527-2
 35.0 MPa
@Strain 2 %,
Temperature 40.0 °C
5080 psi
@Strain 2 %,
Temperature 104 °F
50 mm/min; ISO 527-2
 45.0 MPa
@Strain 2 %,
Temperature 23.0 °C
6530 psi
@Strain 2 %,
Temperature 73.4 °F
50 mm/min; ISO 527-2
 65.0 MPa
@Strain 2 %,
Temperature 0.000 °C
9430 psi
@Strain 2 %,
Temperature 32.0 °F
50 mm/min; ISO 527-2
Tensile Stress at Strain  50.0 MPa
@Strain 8.0 %,
Temperature 60.0 °C
7250 psi
@Strain 8.0 %,
Temperature 140 °F
50 mm/min; ISO 527-2
 50.0 MPa
@Strain 14 %,
Temperature 60.0 °C
7250 psi
@Strain 14 %,
Temperature 140 °F
50 mm/min; ISO 527-2
 60.0 MPa
@Strain 8.0 %,
Temperature 40.0 °C
8700 psi
@Strain 8.0 %,
Temperature 104 °F
50 mm/min; ISO 527-2
 62.0 MPa
@Strain 14 %,
Temperature 40.0 °C
8990 psi
@Strain 14 %,
Temperature 104 °F
50 mm/min; ISO 527-2
 78.0 MPa
@Strain 8.0 %,
Temperature 23.0 °C
11300 psi
@Strain 8.0 %,
Temperature 73.4 °F
50 mm/min; ISO 527-2
 78.0 MPa
@Strain 12 %,
Temperature 23.0 °C
11300 psi
@Strain 12 %,
Temperature 73.4 °F
50 mm/min; ISO 527-2
 95.0 MPa
@Strain 4 %,
Temperature 0.000 °C
13800 psi
@Strain 4 %,
Temperature 32.0 °F
50 mm/min; ISO 527-2
 102 MPa
@Strain 8.0 %,
Temperature 0.000 °C
14800 psi
@Strain 8.0 %,
Temperature 32.0 °F
50 mm/min; ISO 527-2
Elongation at Break 10 %10 %50 mm/min; ISO 37
Charpy Impact Unnotched  7.00 J/cm²
@Temperature -30.0 °C
33.3 ft-lb/in²
@Temperature -22.0 °F
DIN ISO 179
 12.0 J/cm²
@Temperature 23.0 °C
57.1 ft-lb/in²
@Temperature 73.4 °F
DIN ISO 179
Charpy Impact, Notched  1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
DIN ISO 179
 3.00 J/cm²
@Temperature 23.0 °C
14.3 ft-lb/in²
@Temperature 73.4 °F
DIN ISO 179
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
11.1 µin/in-°F
@Temperature 73.4 - 176 °F
53752-A
Deflection Temperature at 0.46 MPa (66 psi) 155 °C311 °FDIN EN ISO 75-2/Be
Deflection Temperature at 1.8 MPa (264 psi) 120 °C248 °FDIN EN ISO 75-2/Ae
Vicat Softening Point 132 °C270 °FB/50; ISO 306
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Processing Temperature 225 - 245 °C437 - 473 °F
Mold Temperature 50.0 - 70.0 °C122 - 158 °F
 
Descriptive Properties
ColorNatural
Commercial StatusNorth America
Primary Processing TechniqueInjection molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Elastollan® 1164D Polyether Type Polyurethane Elastomer
BASF Elastollan® C85A10 (917) Wire & Cable Grade Polyurethane Elastomer
BASF Elastollan® 1085 A TPUR
Alliance Polymers Zythane™ 7085AU Thermoplastic Polyurethane Elastomer
A. Schulman POLYPUR™ FPU 1152C Thermoplastic Polyurethane

PBASG0531 / 132164

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.