MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled
Categories: Polymer; Thermoplastic; Polyketone; Polyaryletherketone (PAEK), Carbon Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.33 - 1.51 g/cc0.0480 - 0.0546 lb/in³Average value: 1.41 g/cc Grade Count:13
Water Absorption 0.0500 - 0.200 %0.0500 - 0.200 %Average value: 0.116 % Grade Count:11
Viscosity  470 - 790 cP
@Temperature 400 - 400 °C
470 - 790 cP
@Temperature 752 - 752 °F
Average value: 600 cP Grade Count:3
 470 - 790 cP
@Shear Rate 1000 - 1000 1/s
470 - 790 cP
@Shear Rate 1000 - 1000 1/s
Average value: 600 cP Grade Count:3
Linear Mold Shrinkage 0.000500 - 0.00900 cm/cm0.000500 - 0.00900 in/inAverage value: 0.00207 cm/cm Grade Count:12
Linear Mold Shrinkage, Transverse 0.00400 - 0.0160 cm/cm0.00400 - 0.0160 in/inAverage value: 0.00882 cm/cm Grade Count:11
Melt Flow 0.800 - 4.50 g/10 min0.800 - 4.50 g/10 minAverage value: 2.45 g/10 min Grade Count:4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 99.0 - 10899.0 - 108Average value: 104 Grade Count:7
Hardness, Shore D 85.0 - 91.085.0 - 91.0Average value: 89.1 Grade Count:4
Tensile Strength, Ultimate 95.0 - 262 MPa13800 - 38000 psiAverage value: 186 MPa Grade Count:11
 45.0 - 160 MPa
@Temperature -50.0 - 250 °C
6530 - 23200 psi
@Temperature -58.0 - 482 °F
Average value: 101 MPa Grade Count:1
Tensile Strength, Yield 95.0 - 821 MPa13800 - 119000 psiAverage value: 333 MPa Grade Count:7
 75.0 - 275 MPa
@Temperature -50.0 - 250 °C
10900 - 39900 psi
@Temperature -58.0 - 482 °F
Average value: 169 MPa Grade Count:1
Elongation at Break 0.800 - 25.0 %0.800 - 25.0 %Average value: 3.17 % Grade Count:13
Modulus of Elasticity 2.96 - 55.8 GPa430 - 8090 ksiAverage value: 23.3 GPa Grade Count:14
Flexural Yield Strength 186 - 894 MPa27000 - 130000 psiAverage value: 347 MPa Grade Count:14
Flexural Modulus 4.20 - 51.4 GPa609 - 7450 ksiAverage value: 18.9 GPa Grade Count:14
Compressive Yield Strength 117 - 574 MPa16900 - 83200 psiAverage value: 264 MPa Grade Count:6
Shear Strength 51.7 - 98.0 MPa7500 - 14200 psiAverage value: 85.9 MPa Grade Count:5
Izod Impact, Notched 0.350 - 0.800 J/cm0.656 - 1.50 ft-lb/inAverage value: 0.573 J/cm Grade Count:12
Izod Impact, Unnotched 3.50 J/cm - NB6.56 ft-lb/in - NBAverage value: 5.75 J/cm Grade Count:11
Izod Impact, Notched (ISO) 8.40 - 9.60 kJ/m²4.00 - 4.57 ft-lb/in²Average value: 8.83 kJ/m² Grade Count:3
Izod Impact, Unnotched (ISO) 37.0 - 39.0 kJ/m²17.6 - 18.6 ft-lb/in²Average value: 38.3 kJ/m² Grade Count:3
Charpy Impact Unnotched 2.00 - 2.00 J/cm²
@Temperature -30.0 - -30.0 °C
9.52 - 9.52 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 2.00 J/cm² Grade Count:1
K (wear) Factor 10100 x 10-8 mm³/N-M5000 x 10-10 in³-min/ft-lb-hrAverage value: 10100 x 10-8 mm³/N-M Grade Count:4
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 20.0 - 1.00e+8 ohm-cm20.0 - 1.00e+8 ohm-cmAverage value: 2.00e+7 ohm-cm Grade Count:6
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.00 - 46.8 µm/m-°C2.78 - 26.0 µin/in-°FAverage value: 14.2 µm/m-°C Grade Count:5
Specific Heat Capacity 1.28 - 1.81 J/g-°C
@Temperature 50.0 - 200 °C
0.306 - 0.433 BTU/lb-°F
@Temperature 122 - 392 °F
Average value: 1.54 J/g-°C Grade Count:3
Thermal Conductivity 0.0370 - 0.600 W/m-K0.257 - 4.16 BTU-in/hr-ft²-°FAverage value: 0.337 W/m-K Grade Count:5
Melting Point 340 - 372 °C644 - 702 °FAverage value: 352 °C Grade Count:8
Deflection Temperature at 1.8 MPa (264 psi) 160 - 368 °C320 - 694 °FAverage value: 289 °C Grade Count:13
Glass Transition Temp, Tg 150 - 343 °C302 - 649 °FAverage value: 179 °C Grade Count:8
Flammability, UL94 V-0V-0Grade Count:7
 
Processing PropertiesMetricEnglishComments
Processing Temperature 390 - 425 °C734 - 797 °FAverage value: 408 °C Grade Count:3
Nozzle Temperature 382 - 425 °C720 - 797 °FAverage value: 401 °C Grade Count:8
Melt Temperature 366 - 420 °C691 - 788 °FAverage value: 379 °C Grade Count:5
Mold Temperature 149 - 220 °C300 - 428 °FAverage value: 188 °C Grade Count:8
Drying Temperature 120 - 150 °C248 - 302 °FAverage value: 146 °C Grade Count:8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyetherimide (PEI)
Overview of materials for Polyetheretherketone, Unreinforced
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
Mitsubishi Chemical Advanced Materials Duratron® CU60 PBI Polybenzimidazole, unfilled, compression molded (ASTM Product Data Sheet)

O2162 / 77941

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.