MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Old Hickory M-44 Kentucky Ball Clay
Categories: Ceramic; Clay; Ball Clay

Material Notes: A highly plastic clay blend containing kaolin and other mixed layer minerals. It is white firing with excellent vitrification properties for use in whiteware ceramic casting, pressing, or plastic forming compositions.

Information provided by Old Hickory Clay Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 0.50 µm0.50 µm44% of particles less than
 0.73 µm0.73 µmMedian particle diameter
 1.0 µm1.0 µm58% of particles less than
 <= 5.0 µm<= 5.0 µm83% of particles less than
pH 6.06.0
Soluble Sulfates 285 ppm285 ppm
Specific Surface Area 25.6 m²/g25.6 m²/g
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00531 GPa0.770 ksiDry Modulus of Rupture for 50% clay/50% flint, cast bars
 
Thermal PropertiesMetricEnglishComments
Shrinkage 5.0 %5.0 %Cone 04, Linear Fired Shrinkage
 5.8 %5.8 %Cone 3, Linear Fired Shrinkage
 6.7 %6.7 %Cone 11, Linear Fired Shrinkage
 6.8 %6.8 %Linear Drying Shrinkage
 
Component Elements PropertiesMetricEnglishComments
Al2O3 27.5 %27.5 %
CaO 0.19 %0.19 %
Fe2O3 1.62 %1.62 %
K2O 1.24 %1.24 %
Loss on Ignition(%) 9.59 %9.59 %
MgO 0.59 %0.59 %
Na2O 0.10 %0.10 %
SiO2 57.68 %57.68 %
TiO2 1.5 %1.5 %
 
Descriptive Properties
Absorption (%)10.1Cone 04, Fired
 3.6Cone 11, Fired
 8.6Cone 3, Fired
CEC/MBI (meg/100 ml)10.4
Crude ColorLight Grey
Filtration (ml)19
Pyrometric Cone Equivalent (PCE)31
Water of Plasticity (%)33
Wet Sieve Residue (%)1.04Wet Sieve Residue, +200 mesh

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

EOHC906 / 161985

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.