MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Envalior Xytron™ G3080E PPS-I-GF30 Polyphenylene Sulfide
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler

Material Notes: Xytron™ offers extremely good chemical resistance, dimensional stability, intrinsic flame retardancy and high stiffness.

Features: 30% Glass Reinforced. Improved Impact. Processing: Injection molding.

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0065 cm/cm0.0065 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  45.0 MPa
@Temperature 200 °C
6530 psi
@Temperature 392 °F
ISO 527-1/-2
 48.0 MPa
@Temperature 160 °C
6960 psi
@Temperature 320 °F
ISO 527-1/-2
 63.0 MPa
@Temperature 120 °C
9140 psi
@Temperature 248 °F
ISO 527-1/-2
 140 MPa
@Temperature 23.0 °C
20300 psi
@Temperature 73.4 °F
ISO 527-1/-2
Elongation at Break  2.5 %
@Temperature 23.0 °C
2.5 %
@Temperature 73.4 °F
ISO 527-1/-2
 6.8 %
@Temperature 120 °C
6.8 %
@Temperature 248 °F
ISO 527-1/-2
 8.5 %
@Temperature 160 °C
8.5 %
@Temperature 320 °F
ISO 527-1/-2
 9.0 %
@Temperature 200 °C
9.0 %
@Temperature 392 °F
ISO 527-1/-2
Tensile Modulus  1.90 GPa
@Temperature 200 °C
276 ksi
@Temperature 392 °F
ISO 527-1/-2
 2.50 GPa
@Temperature 160 °C
363 ksi
@Temperature 320 °F
ISO 527-1/-2
 4.50 GPa
@Temperature 120 °C
653 ksi
@Temperature 248 °F
ISO 527-1/-2
 9.30 GPa
@Temperature 23.0 °C
1350 ksi
@Temperature 73.4 °F
ISO 527-1/-2
Flexural Modulus  2.00 GPa
@Temperature 200 °C
290 ksi
@Temperature 392 °F
ISO 178
 2.80 GPa
@Temperature 160 °C
406 ksi
@Temperature 320 °F
ISO 178
 6.80 GPa
@Temperature 120 °C
986 ksi
@Temperature 248 °F
ISO 178
 7.90 GPa
@Temperature 23.0 °C
1150 ksi
@Temperature 73.4 °F
ISO 178
Izod Impact, Notched (ISO) 16.5 kJ/m²
@Temperature 23.0 °C
7.85 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
@Temperature 23.0 °C
26.2 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1U
Charpy Impact Unnotched  5.50 J/cm²
@Temperature 23.0 °C
26.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
 6.00 J/cm²
@Temperature -30.0 °C
28.6 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  1.10 J/cm²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.60 J/cm²
@Temperature 23.0 °C
7.61 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmIEC 62631-3-1
Dielectric Strength 36.0 kV/mm914 kV/inIEC 60243-1
Comparative Tracking Index 175 V175 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 60.0 µm/m-°C33.3 µin/in-°FISO 11359-1/-2
 110 µm/m-°C61.1 µin/in-°Fabove Tg; ISO 11359-1/-2
CTE, linear, Parallel to Flow 14.0 µm/m-°C7.78 µin/in-°Fabove Tg; ISO 11359-1/-2
 18.0 µm/m-°C10.0 µin/in-°FISO 11359-1/-2
Melting Point 280 °C536 °F10°C/min. Dry; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FISO 75-1/-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSM7960 / 291396

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.