MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

INEOS Styrolution Terlux® 2802 TR Q434 Transparent MABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded

Material Notes: Description: Terlux® 2802 TR Q434 is a new grade with enhanced toughness.

Information provided by STYROLUTION, which is a joint venture between BASF and INEOS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ISO 1183
Water Absorption 0.70 %0.70 %ISO 62
Moisture Absorption at Equilibrium 0.35 %0.35 %23°C/50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/in
Melt Flow  2.16 g/10 min
@Load 10.0 kg,
Temperature 220 °C
2.16 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 18.36 g/10 min
@Load 21.6 kg,
Temperature 220 °C
18.36 g/10 min
@Load 47.6 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8484ISO 2039-2
Ball Indentation Hardness 70.0 MPa
@Load 36.5 kg,
Time 30.0 sec
10200 psi
@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
Tensile Strength, Yield 48.0 MPa6960 psi50mm/min; ISO 527-1/-2
Elongation at Break 12 %12 %Nominal; ISO 527-1/-2
Elongation at Yield 4.0 %4.0 %50mm/min; ISO 527-1/-2
Tensile Modulus 2.00 GPa290 ksiISO 527-1/-2
Charpy Impact Unnotched  12.0 J/cm²
@Temperature -30.0 °C
57.1 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 18.0 J/cm²
@Temperature 23.0 °C
85.7 ft-lb/in²
@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched  0.200 J/cm²
@Temperature -30.0 °C
0.952 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Constant  2.8
@Frequency 1e+6 Hz
2.8
@Frequency 1e+6 Hz
IEC 60250
 2.9
@Frequency 100 Hz
2.9
@Frequency 100 Hz
IEC 60250
Dielectric Strength 34.0 kV/mm864 kV/inK20/P50; IEC 60243-1
Dissipation Factor  0.014
@Frequency 1e+6 Hz
0.014
@Frequency 1e+6 Hz
IEC 60250
 0.016
@Frequency 100 Hz
0.016
@Frequency 100 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 80.0 - 110 µm/m-°C
@Temperature 23.0 - 80.0 °C
44.4 - 61.1 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Maximum Service Temperature, Air 75.0 °C167 °F
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C201 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °FISO 75
Vicat Softening Point 93.0 °C199 °FVST/B/50; ISO 306
 105 °C221 °FVST/A/50; ISO 306
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.541.54ISO 489
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 260 °C446 - 500 °FInjection Molding
Mold Temperature 50.0 - 80.0 °C122 - 176 °FInjection Molding
 
Descriptive Properties
ColorTransparent
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Terlux® 2802 Transparent MABS
INEOS Styrolution Terlux® HD 2802 MABS
INEOS Styrolution Terlux® HD 2812 MABS
INEOS Styrolution Terlux® 2812 Transparent MABS
Barlog Plastics KEBATER A0130 PBT/ABS, 30% glass fiber reinforced, low warpage

PBASG0619 / 132252

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.