MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Abatron AboCast 8503-9/AboCure 8503-9 5-Minute Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: AboCast 8503-9/AboCure 8503-9 is a very-fast-hardening 2-component epoxy adhesive, casting, and patching compound. It is a neutral-buff colored, non-sag, mineral-filled putty to be applied with trowel or other bladed tool for patching, filling, bonding, and anchoring in structural and dielectric applications. It does not have the brittleness typical of conventional 5-minute epoxies. It also provides high resistance to weather, water, salt spray, alkalis, diluted acids, several fuels, solvents, and other chemicals. Unlike other epoxies, a thin layer of this compound does not need any longer to harden than a thick casting.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.70 %
@Time 86400 sec
0.70 %
@Time 24.0 hour
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D  14
@Time 601 sec
14
@Time 0.167 hour
 39
@Time 1800 sec
39
@Time 0.500 hour
 70
@Time 3600 sec
70
@Time 1.00 hour
 78
@Time 86400 sec
78
@Time 24.0 hour
Shear Strength 13.4 MPa1950 psiTensile lap
 
Processing PropertiesMetricEnglishComments
Pot Life 5.0 min5.0 min
Gel Time 5.00 min
@Thickness 1.27 mm
5.00 min
@Thickness 0.0500 in
 
Descriptive Properties
ColorTan
Parts by Weight (pbw)100AboCast 8503-9
 100AboCure 8503-9
ViscosityPutty

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PABC806 / 107790

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.