System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Celanese Impet® 330R PET, 30% Glass Reinforced
Categories:
Polymer
;
Renewable/Recycled Polymer
;
Thermoplastic
;
Polyester, TP
;
Polyethylene Terephthalate (PET)
;
Polyethylene Terephthalate (PET), 30% Glass Reinforced
Material Notes:
Impet 330R is a 30% glass reinforced injection moldable polyester containing post consumer recycled PET. It provides an excellent combination of strength, stiffness, and high temperature resistance.
Information provided by Celanese
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.58
g/cc
1.58
g/cc
ASTM D792
Density
1.58
g/cc
0.0571
lb/in³
ISO 1183
Moisture Absorption
0.160 %
0.160 %
23°C/50%RH; ISO 62
Linear Mold Shrinkage, Flow
0.0020
cm/cm
0.0020
in/in
ISO 294-4
0.0070
cm/cm
0.0070
in/in
ASTM D955
Linear Mold Shrinkage, Transverse
0.0060
cm/cm
0.0060
in/in
ISO 294-4
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell M
122
122
ISO 2039-2
Tensile Strength at Break
159
MPa
23100
psi
5mm/min; ISO 527-2/1A
165
MPa
24000
psi
ASTM D638
Elongation at Break
2.0 %
2.0 %
ASTM D638
2.3 %
2.3 %
5mm/min; ISO 527-2/1A
Tensile Modulus
11.1
GPa
1610
ksi
50mm/min; ISO 527-2/1A
Flexural Strength
229
MPa
33200
psi
ISO 178
245
MPa
35500
psi
ASTM D790
Flexural Modulus
9.65
GPa
1400
ksi
ASTM D790
11.0
GPa
1600
ksi
ISO 178
Izod Impact, Notched
0.801
J/cm
1.50
ft-lb/in
ASTM D256
Izod Impact, Notched (ISO)
8.80
kJ/m²
4.19
ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched
2.70
J/cm²
12.8
ft-lb/in²
ISO 179/1eU
2.80
J/cm²
@Temperature -30.0 °C
13.3
ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched
0.850
J/cm²
4.04
ft-lb/in²
ISO 179/1eA
0.880
J/cm²
@Temperature -30.0 °C
4.19
ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
Electrical Properties
Metric
English
Comments
Volume Resistivity
3.00e+15
ohm-cm
3.00e+15
ohm-cm
ASTM D257
7.00e+16
ohm-cm
7.00e+16
ohm-cm
IEC 60093
Surface Resistance
3.10e+14
ohm
3.10e+14
ohm
ASTM D257
3.00e+15
ohm
3.00e+15
ohm
IEC 60093
Dielectric Constant
2.83
@Frequency 100 Hz
2.83
@Frequency 100 Hz
IEC 60250
3.1
@Frequency 10000 Hz
3.1
@Frequency 10000 Hz
ASTM D150
3.2
@Frequency 1000 Hz
3.2
@Frequency 1000 Hz
ASTM D150
3.46
@Frequency 1e+6 Hz
3.46
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength
22.2
kV/mm
565
kV/in
short term; ASTM D149
32.0
kV/mm
813
kV/in
IEC 60243-1
Dissipation Factor
0.010
@Frequency 1000 Hz
0.010
@Frequency 1000 Hz
ASTM D150
0.012
@Frequency 100 Hz
0.012
@Frequency 100 Hz
IEC 60250
0.014
@Frequency 1e+6 Hz
0.014
@Frequency 1e+6 Hz
IEC 60250
0.016
@Frequency 10000 Hz
0.016
@Frequency 10000 Hz
ASTM D150
Arc Resistance
125
sec
125
sec
ASTM D495
Comparative Tracking Index
175
V
175
V
ASTM D3638
175
V
175
V
IEC 60112
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
18.0
µm/m-°C
10.0
µin/in-°F
ISO 11359-2
CTE, linear, Transverse to Flow
70.0
µm/m-°C
38.9
µin/in-°F
ISO 11359-2
Melting Point
244
°C
471
°F
10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi)
240
°C
464
°F
ISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi)
221
°C
430
°F
ISO 75-1, -2
224
°C
435
°F
ASTM D648
Glass Transition Temp, Tg
73.0
°C
163
°F
ISO 11357-1,-2,-3
Flammability, UL94
HB
HB
Oxygen Index
25 %
25 %
ISO 4589
Processing Properties
Metric
English
Comments
Processing Temperature
110
-
121
°C
230
-
250
°F
cavity
260
-
290
°C
500
-
554
°F
hot runner
Feed Temperature
255
-
265
°C
491
-
509
°F
Zone 1
255
-
265
°C
491
-
509
°F
Zone 2
260
-
275
°C
500
-
527
°F
Zone 3
260
-
275
°C
500
-
527
°F
Zone 4
265
-
280
°C
509
-
536
°F
Die Temperature
270
-
290
°C
518
-
554
°F
Melt Temperature
260
-
290
°C
500
-
554
°F
285
°C
545
°F
ISO 294
Mold Temperature
135
°C
275
°F
ISO 294
Injection Velocity
275
mm/sec
10.8
in/sec
ISO 294
Drying Temperature
130
-
140
°C
266
-
284
°F
Dry Time
4.00
hour
4.00
hour
Moisture Content
<= 0.010 %
<= 0.010 %
Hold Pressure
60.0
MPa
8700
psi
ISO 294
Descriptive Properties
Injection molding
Yes
Injection speed
medium-fast
Processing conditions acc. ISO
7792-2
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
VICTREX™ PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
EMS-Grivory Grivory® XE 4101 black 9225 PA*-GF40
DuPont Mobility and Materials Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)
PHCQ443 / 178898
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.