MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Mitsubishi Chemical Advanced Materials Nylatron™ GSM PA6 Nylon, Cast MoS2 Filled Type 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, MoS2 Filled

Material Notes: An impact-resistant cast nylon with finely divided particles of MoS2 to enhance load-bearing capabilities. Exhibits ideal combination of strength and toughness, as well as mechanical and electrical properties.

Key Words: Polyamide 6; PA6; PA 6
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/ccASTM D792
Water Absorption at Saturation 7.00 %7.00 %ASTM D570 (17)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 84.084.0ASTM D785
Hardness, Shore D 80.080.0ISO 868
Tensile Strength 82.0 MPa11900 psiISO 527-1/-2 (7)
Elongation at Yield 5.00 %5.00 %ISO 527-1/-2 (7)
Flexural Strength 111 MPa16100 psiISO 178 (12)
Compressive Yield Strength  33.0 MPa
@Strain 1.00 %
4790 psi
@Strain 1.00 %
ISO 604 (10)
 62.0 MPa
@Strain 2.00 %
8990 psi
@Strain 2.00 %
ISO 604 (10)
 91.0 MPa
@Strain 5.00 %
13200 psi
@Strain 5.00 %
ISO 604 (10)
Shear Strength 72.0 MPa10400 psiASTM D732
Charpy Impact, Notched 0.300 J/cm²1.43 ft-lb/in²ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+14 ohm1.00e+14 ohmANSI/ESD STM 11.11
Dielectric Constant 3.70
@Frequency 1.00e+6 Hz
3.70
@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 15.7 kV/mm400 kV/inASTM D149
 24.0 kV/mm610 kV/inIEC 60243-1 (15)
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°FASTM E-831 (TMA)
 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 140 °F
 90.0 µm/m-°C
@Temperature 23.0 - 100 °C
50.0 µin/in-°F
@Temperature 73.4 - 212 °F
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°F
Melting Point 216 °C420 °FASTM D3418
Maximum Service Temperature, Air 93.3 °C200 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 93.3 °C200 °FASTM D648
Minimum Service Temperature, Air -30.0 °C-22.0 °F
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) LimitedLimited
Acids, Weak LimitedLimited
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Continuous Sunlight AcceptableAcceptable
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Nylatron™ GSM Blue PA6 Cast Oil & MoS2 Filled Type 6
Mitsubishi Chemical Advanced Materials Nylatron™ MC 901 H.S. PA6
Mitsubishi Chemical Advanced Materials Nylatron™ NSM PA6 Nylon, Cast Solid Lubricant Filled, Type 6
Mitsubishi Chemical Advanced Materials Nylatron™ GS PA66 with MoS2, extruded
Mitsubishi Chemical Advanced Materials Nylatron™ MC™ 907 / Ertalon™ 6 PLA PA6 Unfilled Type 6 nylon

P1SM23 / 20109

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.