MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

BASF Ultramid® A3W2G7 BK20560 PA66+6, 35% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 40% Glass Fiber Reinforced

Material Notes: Ultramid A3W2G7 BK20560 is a 35% glass fiber reinforced, pigmented black, injection molding PA66+PA6 with high heat aging resistance.

Applications: Applications include automotive powertrain applications like charge air coolers.

Information provided by BASF.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³ISO 1183
Moisture Absorption 1.50 %1.50 %50% RH; ISO 62
Water Absorption at Saturation 5.0 %5.0 %ISO 62
Linear Mold Shrinkage, Flow 0.031 cm/cm0.031 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.085 cm/cm0.085 in/inISO 294-4
Melt Flow 30 g/10 min
@Load 5.00 kg,
Temperature 275 °C
30 g/10 min
@Load 11.0 lb,
Temperature 527 °F
Dry; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 115 MPa16700 psiConditioned; ISO 527
 205 MPa29700 psiDry; ISO 527
Elongation at Break 3.2 %3.2 %Dry; ISO 527
 6.0 %6.0 %Conditioned; ISO 527
Tensile Modulus 6.50 GPa943 ksiConditioned; ISO 527
 11.3 GPa1640 ksiDry; ISO 527
Flexural Strength 180 MPa26100 psiConditioned; ISO 178
 305 MPa44200 psiDry; ISO 178
Flexural Modulus 6.10 GPa885 ksiConditioned; ISO 178
 10.4 GPa1510 ksiDry; ISO 178
Charpy Impact Unnotched  7.50 J/cm²
@Temperature -30.0 °C
35.7 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179
 9.50 J/cm²
@Temperature 23.0 °C
45.2 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179
 10.5 J/cm²
@Temperature 23.0 °C
50.0 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179
 80.1 J/cm²
@Temperature -30.0 °C
381 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179
Charpy Impact, Notched  0.900 J/cm²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179
 0.900 J/cm²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179
 1.10 J/cm²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179
 1.80 J/cm²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FDry; ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 255 °C491 °FDry; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 235 °C455 °FDry; ISO 75
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 305 °C536 - 581 °F
Mold Temperature 45.0 - 105 °C113 - 221 °Fcan be used where applicable
 80.0 - 90.0 °C176 - 194 °Frecommended
 80.0 - 90.0 °C176 - 194 °F
Drying Temperature 80.0 °C
@Time 7200 - 14400 sec
176 °F
@Time 2.00 - 4.00 hour
Moisture Content <= 0.15 %<= 0.15 %
Injection Pressure 3.45 - 10.3 MPa500 - 1500 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASF8948 / 254906

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.