MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Mitsubishi Chemical Advanced Materials Sultron™ LSG PSU Extruded, Unfilled, Polysulfone (ASTM Product Data Sheet)
Categories: Polymer; Thermoplastic; Polysulfone (PSU)

Material Notes:

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.24 g/cc1.24 g/ccASTM D792
Water Absorption 0.30 %0.30 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 0.60 %0.60 %Immersion; ASTM D570(2)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8282ASTM D785
Hardness, Rockwell R 128128ASTM D785
Hardness, Shore D 8080ASTM D2240
Tensile Strength 70.3 MPa10200 psiASTM D638
Tensile Strength at 150°C (300°F) 41.4 MPa6000 psiASTM D638
Tensile Strength at 65°C (150°F) 55.2 MPa8000 psiASTM D638
Elongation at Break 30 %30 %ASTM D638
Tensile Modulus 2.69 GPa390 ksiASTM D638
Flexural Strength 103 MPa15000 psiASTM D790
Flexural Modulus 2.76 GPa400 ksiASTM D790
Compressive Strength 89.6 MPa13000 psi10% Def.; ASTM D695
Compressive Modulus 2.59 GPa375 ksiASTM D695
Shear Strength 62.1 MPa9000 psiASTM D732
Izod Impact, Notched 0.694 J/cm1.30 ft-lb/inASTM D256 Type A
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+13 ohm>= 1.00e+13 ohmEOS/ESD S11.11
Dielectric Constant 3.14
@Frequency 1e+6 Hz
3.14
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 16.7 kV/mm425 kV/inShort Term; ASTM D149
Dissipation Factor 0.00080
@Frequency 1e+6 Hz
0.00080
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.8 µm/m-°C
@Temperature -40.0 - 149 °C
31.0 µin/in-°F
@Temperature -40.0 - 300 °F
ASTM E831
Thermal Conductivity 0.259 W/m-K1.80 BTU-in/hr-ft²-°FASTM F433
Maximum Service Temperature, Air 149 °C300 °FLong Term
Deflection Temperature at 1.8 MPa (264 psi) 171 °C340 °FASTM D648
Glass Transition Temp, Tg 190 °C374 °FASTM D3418
Flammability, UL94 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
Estimated Rating
 
Compliance PropertiesMetricEnglishComments
3A-Dairy YesYes
Canada AG NoNo
FDA YesYes
NSF YesYesSTD 61
USDA YesYes
USP Class VI YesYes
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) UnacceptableUnacceptable
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) UnacceptableUnacceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents UnacceptableUnacceptable
Conductive / Static Dissipative NoNo
Continuous Sunlight LimitedLimited
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic LimitedLimited
Hydrocarbons - Aromatic UnacceptableUnacceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters UnacceptableUnacceptable
 
Descriptive Properties
ColorNatural
Machinability31-10, 1=Easier to Machine

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Sultron™ PSU Extruded Unfilled Polysulfone (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Acetron® GP Copolymer Acetal, Porosity-Free, Unfilled, Extruded (ASTM datasheet)
Mitsubishi Chemical Advanced Materials TIVAR® 1000 UHMW-PE, (Natural & Colors except Black) (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Acetron® MD Metal-detectable Copolymer Acetal (ASTM Product Data Sheet)
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded

P1SM50A1 / 129699

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.