MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Evonik Vestoran® 1900 PPE Compound  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, Molded

Material Notes: Description: The polyphenylene ether compounds (PPE) VESTORAN® are amorphous materials with high heat deflection temperature. VESTORAN® compounds and the parts produced from them have the following properties:
  • very low water absorption
  • hot water-resistant
  • resistant to alkalis and acids
  • very low mold shrinkage
  • very low tendency to warp

VESTORAN® has proved to be highly suitable for production of coil bodies for vehicle electricity on account of its high dimensional stability, heat deflection temperature, dielectric strength, and ability to bond well to insulating compounds (epoxy resins). In addition, its low water absorption makes it a good choice for producing impellers for water pumps, for example, in engine cooling, but also for applications in machinery and engineering. Further applications include relay sockets, distributor cabinets, and large capacitor cases.

Applications: Vibration absorbers, shock absorbing bushings, reinforced profiles, seals

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Water Absorption at Saturation 0.40 %0.40 %ISO 62
Linear Mold Shrinkage 0.009 cm/cm
@Thickness 2.00 mm
0.009 in/in
@Thickness 0.0787 in
sheet with film gate at rim, mold temperature 80°C
Linear Mold Shrinkage, Transverse 0.008 cm/cm
@Thickness 2.00 mm
0.008 in/in
@Thickness 0.0787 in
sheet with film gate at rim, mold temperature 80°C
High Load Melt Index >= 20.8 g/10 min
@Load 21.6 kg,
Temperature 300 °C
>= 20.8 g/10 min
@Load 47.6 lb,
Temperature 572 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.0 MPa8700 psiISO 527-1/2
Elongation at Break >= 50 %>= 50 %ISO 527-1/2
Elongation at Yield 6.0 %6.0 %ISO 527-1/2
Tensile Modulus 2.00 GPa290 ksiISO 527-1/2
Flexural Modulus 2.40 GPa348 ksiISO 178
Charpy Impact Unnotched 25.0 J/cm²
@Temperature 23.0 °C
119 ft-lb/in²
@Temperature 73.4 °F
Partial Break; ISO 179/1eU
Charpy Impact, Notched 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance 2.00e+14 ohm2.00e+14 ohmIEC 60093
Dielectric Constant  2.6
@Frequency 100 Hz
2.6
@Frequency 100 Hz
IEC 60250
 2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 40.0 kV/mm1020 kV/inK20/P50; IEC 60243-1
Dissipation Factor  0.00080
@Frequency 100 Hz
0.00080
@Frequency 100 Hz
IEC 60250
 0.0016
@Frequency 1e+6 Hz
0.0016
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 200 V200 VTest Solution A, 100 drops; IEC 60112
 225 V225 VTest Solution A, CTI; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) >= 190 °C>= 374 °FISO 75-1/2
Deflection Temperature at 1.8 MPa (264 psi) >= 170 °C>= 338 °FISO 75-1/2
Vicat Softening Point >= 185 °C>= 365 °F50N; ISO 306
 >= 190 °C>= 374 °F10N; ISO 306
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Descriptive Properties
ColorNatural, Black
Electrolytic CorrosionA1 StepIEC 60426

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik Vestoran® 1100 nf PPE
Lehmann & Voss LUVOCOM® 1105/CF/10/GR/10/TF/10-2 PEEK with carbon fiber, PTFE, lubricant modified
Mitsubishi Iupiace® EHM1010A m-Polyphenylene Ether (m-PPE)
BLUESTAR LXS 312 PPE-HIPS, 20% Mineral Filled
Evonik Vestodur® X7061 Laser Markable PBT

PHUMA80 / 47594

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.