MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Overview of materials for Polysulfone, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polysulfone (PSU); Polysulfone, 20% Glass Fiber Reinforced

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.33 - 1.47 g/cc0.0480 - 0.0531 lb/in³Average value: 1.40 g/cc Grade Count:15
Filler Content 15.0 - 20.0 %15.0 - 20.0 %Average value: 19.0 % Grade Count:5
Water Absorption 0.200 - 0.700 %0.200 - 0.700 %Average value: 0.320 % Grade Count:8
Linear Mold Shrinkage 0.00150 - 0.00800 cm/cm0.00150 - 0.00800 in/inAverage value: 0.00352 cm/cm Grade Count:14
Linear Mold Shrinkage, Transverse 0.00520 - 0.00850 cm/cm0.00520 - 0.00850 in/inAverage value: 0.00657 cm/cm Grade Count:3
Melt Flow 6.50 - 40.0 g/10 min6.50 - 40.0 g/10 minAverage value: 16.9 g/10 min Grade Count:4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120 - 123120 - 123Average value: 122 Grade Count:6
Tensile Strength, Ultimate 62.1 - 115 MPa9000 - 16700 psiAverage value: 96.0 MPa Grade Count:13
 50.0 - 90.0 MPa
@Temperature 60.0 - 150 °C
7250 - 13100 psi
@Temperature 140 - 302 °F
Average value: 71.3 MPa Grade Count:2
Tensile Strength, Yield 97.9 - 112 MPa14200 - 16200 psiAverage value: 107 MPa Grade Count:3
Elongation at Break 0.500 - 7.00 %0.500 - 7.00 %Average value: 3.08 % Grade Count:15
 1.80 - 2.50 %
@Temperature 60.0 - 150 °C
1.80 - 2.50 %
@Temperature 140 - 302 °F
Average value: 2.16 % Grade Count:2
Modulus of Elasticity 2.55 - 7.00 GPa370 - 1020 ksiAverage value: 5.75 GPa Grade Count:13
 4.70 - 5.80 GPa
@Temperature 60.0 - 150 °C
682 - 841 ksi
@Temperature 140 - 302 °F
Average value: 5.30 GPa Grade Count:2
Flexural Yield Strength 82.7 - 176 MPa12000 - 25500 psiAverage value: 143 MPa Grade Count:13
Flexural Modulus 2.41 - 6.70 GPa350 - 972 ksiAverage value: 5.50 GPa Grade Count:12
Shear Modulus 0.0250 - 0.950 GPa
@Temperature 50.0 - 200 °C
3.63 - 138 ksi
@Temperature 122 - 392 °F
Average value: 0.669 GPa Grade Count:1
Izod Impact, Notched 0.530 - 1.07 J/cm0.993 - 2.00 ft-lb/inAverage value: 0.708 J/cm Grade Count:12
Izod Impact, Unnotched 3.35 - 6.94 J/cm6.28 - 13.0 ft-lb/inAverage value: 5.18 J/cm Grade Count:9
Izod Impact, Notched (ISO) 7.00 - 7.00 kJ/m²
@Temperature -30.0 - -30.0 °C
3.33 - 3.33 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 7.00 kJ/m² Grade Count:1
Charpy Impact Unnotched 3.00 - 4.50 J/cm²14.3 - 21.4 ft-lb/in²Average value: 3.50 J/cm² Grade Count:3
 4.00 - 4.50 J/cm²
@Temperature -30.0 - -20.0 °C
19.0 - 21.4 ft-lb/in²
@Temperature -22.0 - -4.00 °F
Average value: 4.25 J/cm² Grade Count:2
Charpy Impact, Notched 0.350 - 0.800 J/cm²1.67 - 3.81 ft-lb/in²Average value: 0.617 J/cm² Grade Count:3
 0.350 - 0.750 J/cm²
@Temperature -30.0 - -20.0 °C
1.67 - 3.57 ft-lb/in²
@Temperature -22.0 - -4.00 °F
Average value: 0.550 J/cm² Grade Count:2
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+12 - 2.00e+16 ohm-cm1.00e+12 - 2.00e+16 ohm-cmAverage value: 6.11e+15 ohm-cm Grade Count:11
Surface Resistance 1.00e+14 ohm1.00e+14 ohmAverage value: 1.00e+14 ohm Grade Count:3
Dielectric Constant 3.00 - 3.503.00 - 3.50Average value: 3.32 Grade Count:3
Dielectric Strength 16.7 - 46.0 kV/mm425 - 1170 kV/inAverage value: 22.6 kV/mm Grade Count:6
Dissipation Factor 0.00100 - 0.008000.00100 - 0.00800Average value: 0.00480 Grade Count:3
Comparative Tracking Index 125 V125 VAverage value: 125 V Grade Count:3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 26.0 - 55.8 µm/m-°C14.4 - 31.0 µin/in-°FAverage value: 35.8 µm/m-°C Grade Count:4
 28.0 - 28.0 µm/m-°C
@Temperature 140 - 180 °C
15.6 - 15.6 µin/in-°F
@Temperature 284 - 356 °F
Average value: 28.0 µm/m-°C Grade Count:1
Maximum Service Temperature, Air 160 - 180 °C320 - 356 °FAverage value: 166 °C Grade Count:4
Deflection Temperature at 0.46 MPa (66 psi) 181 - 188 °C358 - 370 °FAverage value: 185 °C Grade Count:6
Deflection Temperature at 1.8 MPa (264 psi) 174 - 260 °C345 - 500 °FAverage value: 190 °C Grade Count:14
Glass Transition Temp, Tg 185 - 265 °C365 - 509 °FAverage value: 221 °C Grade Count:4
Flammability, UL94 HB - V-0HB - V-0Grade Count:11
Oxygen Index 35.0 - 40.0 %35.0 - 40.0 %Average value: 37.7 % Grade Count:3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 300 - 410 °C572 - 770 °FAverage value: 358 °C Grade Count:10
Mold Temperature 93.3 - 210 °C200 - 410 °FAverage value: 146 °C Grade Count:12
Drying Temperature 110 - 170 °C230 - 338 °FAverage value: 143 °C Grade Count:9
Moisture Content 0.150 %0.150 %Average value: 0.150 % Grade Count:4
Dew Point -31.7 °C-25.0 °FAverage value: -31.7 °C Grade Count:4
Injection Pressure 68.9 - 124 MPa10000 - 18000 psiAverage value: 96.5 MPa Grade Count:6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger TECASINT 5051 Polyimide, 30% Glass Fiber Filled (PI)
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled
BASF Ultrason® E 3010 PES
Overview of materials for Polysulfone (PSU)
BASF Ultramid® B3EG6 BK00564 30% Glass Filled PA6 (Dry)

O5312 / 78483

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.