System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
CENTROPLAST CENTROMID 12 soft Polyamide 12 soft
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 12 (PA12)
;
Nylon 12, Extrusion/Tubing Grade
Material Notes:
This extruded material is suitable for conveying foodstuffs and pharmaceutical products. It is used in flexible tubes for worm gears and spiral conveyors.
Information provided by CENTROPLAST Engineering Plastics GMBH
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.03
g/cc
0.0372
lb/in³
ISO 1183
Moisture Absorption at Equilibrium
0.50 %
0.50 %
in normal climate 23°C/50%RH; ISO 62
Water Absorption at Saturation
1.0 %
1.0 %
in water at 23°C; ISO 62
Mechanical Properties
Metric
English
Comments
Ball Indentation Hardness
64.0
MPa
9280
psi
value at 30 sec.; ISO 2039-1
Tensile Strength, Yield
25.0
MPa
3630
psi
v = 50 mm/min; ISO 527-2
Elongation at Break
>= 50 %
>= 50 %
ISO 527-2
Tensile Modulus
0.400
GPa
58.0
ksi
ISO 527-2
Charpy Impact Unnotched
NB
NB
ISO 179/1eU
Charpy Impact, Notched
NB
NB
ISO 179/1eA
Electrical Properties
Metric
English
Comments
Electrical Resistivity
1.00e+12
ohm-cm
1.00e+12
ohm-cm
IEC 60093
Surface Resistance
1.00e+12
ohm
1.00e+12
ohm
IEC 60093
Dielectric Constant
3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength
31.0
kV/mm
787
kV/in
in transformer oil; IEC 60243-1
Comparative Tracking Index
575
V
575
V
IEC 60112
Thermal Properties
Metric
English
Comments
Melting Point
171
°C
340
°F
10K/min; ISO 3146
Maximum Service Temperature, Air
75.0
°C
167
°F
Long Term
125
°C
257
°F
Short term
Deflection Temperature at 1.8 MPa (264 psi)
125
-
165
°C
257
-
329
°F
ISO 75-2
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Overview of materials for Nylon 12
Overview of materials for Acrylic, General Purpose, Molded
GEHR Plastics PA 12 TR Transparent Nylon 12
CENTROPLAST CENTROTRON GF 15 Polyphenylene sulfide 15% glass fiber
CENTROPLAST CENTROMID 6.6 CF 20 Polyamide 6.6 carbon fiber
PCENTR15 / 27966
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.