MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Techmer ES Electrablend® PA6/6 03001 Carbon Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 10% Carbon Fiber Filled; Nylon 66, Conductive; Nylon 66, Heat Stabilized; Nylon 66, Impact Grade

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Carbon Fiber Reinforcement

Additive: Impact Modifier and Heat Stabilizer

Features: Electrically Conductive, Impact Modified and Heat Stabilized

Information provided by TP Composites, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ASTM D792
Water Absorption 0.90 %
@Time 86400 sec
0.90 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.010 cm/cm
@Thickness 3.17 mm
0.010 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 111111ASTM D785
Tensile Strength, Yield 121 MPa17500 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Flexural Strength 165 MPa24000 psiASTM D790
Flexural Modulus 8.27 GPa1200 ksiASTM D790
Izod Impact, Notched 1.92 J/cm
@Thickness 3.17 mm
3.60 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 10.1 J/cm
@Thickness 3.17 mm
19.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 10000 - 1.00e+6 ohm-cm10000 - 1.00e+6 ohm-cmASTM D257
Surface Resistance 10000 - 1.00e+6 ohm10000 - 1.00e+6 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 39.6 µm/m-°C22.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 252 °C485 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 220 °C428 °FUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 399 X 95997 B Polycarbonate (PC), Thermally Conductive - Electrically Conductive
RTP Company RTP 299 X 127044 D Nylon 6/6 (PA); Thermally Conductive - Flame Retardant
RTP Company RTP 299 X 124222 B Nylon 6/6 (PA); Thermally Conductive - Electrically Conductive - Flame Retardant - Preliminary
RTP Company RTP 2799S X 89622 C  Styrenic Thermoplastic Elastomer (TES) Thermally Conductive - Electrically Conductive - SEBS
RTP Company RTP 2299 X 108681 Polyetheretherketone (PEEK) Thermally Conductive - Electrically Insulative - Abrasive

PTPC0997 / 136935

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.