MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Ineos G50-120 HDPE, Sheet Extrusion Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Sheet/Thermoforming Grade

Material Notes: G50-120 is a high molecular weight, high density polyethylene copolymer developed for sheet extrusion and thermoforming where the finished product demands outstanding physical performance. This material meets the Food and Drug Administration requirements of 21CFR 177.1520.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ASTM D4883
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 190 °C
12 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ASTM D2240
Tensile Strength, Ultimate 30.3 MPa4390 psiASTM D638
Tensile Strength, Yield 27.6 MPa4000 psiASTM D638
Elongation at Break >= 800 %>= 800 %ASTM D638
Tensile Modulus 0.930 GPa135 ksiASTM D638
Flexural Modulus 0.970 GPa141 ksiTangent-Method 1; ASTM D790
Tensile Impact Strength 505 kJ/m²240 ft-lb/in²Type L; ASTM D 1822
 
Thermal PropertiesMetricEnglishComments
CTE, linear 120 µm/m-°C
@Temperature 20.0 °C
66.7 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C167 °FASTM D648
Vicat Softening Point 130 °C266 °FASTM D1525
Brittleness Temperature <= -75.0 °C<= -103 °FASTM D746
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos G60-25-144 HDPE
Ineos T60-1200-119 HDPE
Ineos TC46-25 HDPE
Ineos H02C-01 Polypropylene Homopolymer
Ineos H02C-00 Polypropylene Homopolymer

PSOLJA / 68180

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.