MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Celanese ZENITE 6330 LCP, 30% Mineral Reinforced
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), Mineral Filled

Material Notes: Zenite« 6330 is a 30% mineral reinforced liquid crystal polymer for injection molding. It has excellent impact resistance, excellent heat deflection temperature and and is well suited for all kinds of demanding applications.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.64 g/cc0.0592 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.00 cm/cm0.00 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0065 cm/cm0.0065 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 130 MPa18900 psi5mm/min; ISO 527-2/1A
Elongation at Break 5.0 %5.0 %5mm/min; ISO 527-2/1A
Tensile Modulus 10.0 GPa1450 ksi50mm/min; ISO 527-2/1A
Flexural Modulus 9.50 GPa1380 ksiISO 178
Charpy Impact Unnotched 6.00 J/cm²28.6 ft-lb/in²ISO 179/1eU
 4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²4.28 ft-lb/in²ISO 179/1eA
 0.800 J/cm²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 60093
Dielectric Constant  3.4
@Frequency 1e+6 Hz
3.4
@Frequency 1e+6 Hz
IEC 60250
 3.8
@Frequency 100 Hz
3.8
@Frequency 100 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm889 kV/inIEC 60243-1
Dissipation Factor  0.014
@Frequency 100 Hz
0.014
@Frequency 100 Hz
IEC 60250
 0.031
@Frequency 1e+6 Hz
0.031
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 200 V200 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 8.00 µm/m-°C4.44 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 40.0 µm/m-°C22.2 µin/in-°FISO 11359-2
Melting Point 335 °C635 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 275 °C527 °FISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 245 °C473 °FISO 75-1, -2
Glass Transition Temp, Tg 120 °C248 °FISO 11357-1,-2,-3
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 0.850 mm
V-0
@Thickness 0.0335 in
Oxygen Index 47 %47 %ISO 4589
 
Processing PropertiesMetricEnglishComments
Processing Temperature 40.0 - 150 °C104 - 302 °Fcavity
Melt Temperature 350 - 360 °C662 - 680 °F
Drying Temperature >= 150 °C>= 302 °F
Dry Time 3.00 hour3.00 hour
Moisture Content <= 0.010 %<= 0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zenite® 6330 BK010 LCP (Extended Tabular Temperature Data)
Celanese ZENITE 6130L LCP, 30% Glass Reinforced
Celanese ZENITE 6130 LCP, 30% Glass Reinforced
Celanese ZENITE 6635 LCP, 40% Mineral / Glass Reinforced (Extended Stress-Strain Tabular Data)
Celanese Zenite® 6330 NC010 LCP (Extended Tabular Temperature Data)

PHCQ540 / 178995

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.