MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Evonik VESTOPLAST® 206 B Amorphous Polyalphaolefin
Categories: Polymer; Thermoplastic; Polyalphaolefin

Material Notes: VESTOPLAST 206 is a reactive, silane grafted, amorphous polyalphaolefin. It causes a high adhesion to substrates such as glass, ceramics, metals and polar plastics.

Key Words: APAO
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.870 g/cc
@Temperature 23.0 °C
0.0314 lb/in³
@Temperature 73.4 °F
DIN 53 482
Viscosity 6000 cP
@Temperature 190 °C
6000 cP
@Temperature 374 °F
melt; DIN 53 019
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 1.90 MPa276 psiDIN EN ISO 527-3
Elongation at Break 720 %720 %DIN EN ISO 527-3
Penetration 20
@Thickness 0.100 mm
20
@Thickness 0.00394 in
needle 100/25/5; DIN 52 010
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -34.0 °C-29.2 °FDIN 53 765
Ring & Ball Softening Point 104 °C219 °FDIN 52 011
 
Descriptive Properties
Open Time (sec)50Degussa Method
Setting Time (sec)1Degussa Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik VESTOPLAST® 206 + 6%, 206 B Amorphous Polyalphaolefin
Evonik VESTOPLAST® EP NC 702 Amorphous Polyalphaolefin
Evonik VESTOPLAST® 750 Amorphous Polyalphaolefin
Evonik VESTOPLAST® 708 Amorphous Polyalphaolefin
Evonik VESTOPLAST® 704 Amorphous Polyalphaolefin

PHUMB410 / 81412

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.