MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik VESTAPE® PA12-CF45 Nylon 12, Carbon Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Carbon Fiber Filled

Material Notes: HT carbon fiber reinforced UD-tape made from polyamide 12 . VESTAPE® PA12-CF45 is an unidirectional carbon fiber reinforced tape made from PA12 with a fiber volume content of 45 %, that shows a high chemical resistance, low water absorption and steady mechanical properties over a wide temperature range. VESTAPE® PA12-CF45 is supplied as a band-shaped semi-finished product showing a width of 160 mm and a thickness of 0,25 mm.

Property data for dry samples.

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ISO 1183
Filler Content 45 %45 %Volume. Tape property; EN 2559
 59 %59 %Weight Tape property; EN 2559
Moisture Absorption 0.470 %0.470 %Sim. to ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 35.0 MPa5080 psiLaminate property. 90° Orientation; ISO 527-5
 1750 MPa254000 psiTape property. 0° Orientation; Sim. to. ISO 527-5
 1750 MPa254000 psiLaminate property. 0° Orientation; ISO 527-5
Elongation at Break 1.8 %1.8 %Tape property. 0° Orientation; Sim. to. ISO 527-5
Tensile Modulus 4.50 GPa653 ksiLaminate property. 90° Orientation; ISO 527-5
 100 GPa14500 ksiLaminate property. 0° Orientation; ISO 527-5
 100 GPa14500 ksiTape property. 0° Orientation; Sim. to. ISO 527-5
Flexural Strength 60.0 MPa8700 psi90°, Laminate property; ISO 14125
 900 MPa131000 psi0°, Laminate property; ISO 14125
Flexural Modulus 4.50 GPa653 ksi90°, Laminate property; ISO 14125
 95.0 GPa13800 ksi0°. Laminate property; ISO 14125
Compressive Strength 45.0 MPa6530 psi0°. Laminate property; ISO 14126
Shear Modulus 1.40 GPa203 ksiG12. Laminate property; ISO 14129
Shear Strength 30.0 MPa4350 psiPerpendicular. 12M, 23°C. Laminate property; ISO 14129
 45.0 MPa6530 psiInterlaminar; ISO 14130
 
Thermal PropertiesMetricEnglishComments
Melting Point 178 °C352 °FISO 11357-1/-3
Glass Transition Temp, Tg 40.0 °C104 °FISO 11357-1/-2
 
Descriptive Properties
Tape Areal Weight343 g/m2
Tape Thickness0.25 mm
Tape Width160 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK877 / 243084

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.