MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Eurotec® Tecodur® PB70 GR30 NL MB04 PBT/ASA, 30% glass fiber reinforced, heat & UV stabilized, natural
Categories: Polymer; Thermoplastic; ASA Polymer; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + ASA Blend, Glass Fiber Reinforced; Polybutylene Terephthalate (PBT), Heat Resistant

Material Notes:

Information provided by Eurotec®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ISO 1183
Moisture Absorption 0.100 %
@Temperature 23.0 °C
0.100 %
@Temperature 73.4 °F
50% RH; ISO 960
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inEurotec
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inEurotec
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 120 MPa17400 psiISO 527
Elongation at Break 2.5 %2.5 %ISO 527
Tensile Modulus 9.50 GPa1380 ksiISO 527
Izod Impact, Notched (ISO)  9.00 kJ/m²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 11.0 kJ/m²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °F[10 K/min], ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 155 °C311 °FISO 75
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 250 - 270 °C482 - 518 °F
Feed Temperature 50.0 - 70.0 °C122 - 158 °FThroat
Mold Temperature 60.0 - 100 °C140 - 212 °F
Drying Temperature 120 °C248 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Moisture Content <= 0.080 %<= 0.080 %ISO 960
Hold Pressure 40.0 - 80.0 MPa5800 - 11600 psi
 
Descriptive Properties
Back PressureLow
Injection SpeedFast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Pocan® A 3131 000000 PBT+PC, 30% Glass Fiber Reinforced
Eurotec® Tecodur® PB70 NL IL PBT, impact modified, natural
Celanese Crastin® LW9030 BK851 PBT+ASA-GF30
Celanese Crastin® LW9020FR BK851 PBT+ASA-GF20FR(17)
BASF Ultradur® S 4090 G6X 30% Glass Filled PBT + ASA

PEUROS110 / 147100

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.