MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Plenco 7021 Phenolic, Granular, Injection Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Impact Grade, Filled

Material Notes: PLENCO 07021 is a renumber of Plaslok 7021 which is the replacement material for the former Union Carbide BMRS-7021. It is a two-stage, impact grade phenolic molding compound suitable for compression, transfer or injection molding of switchgear parts, or where mechanical assembly requires better impact strength. PLENCO 07021 is UL recognized under component file E40654.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.460 g/cc0.0166 lb/in³ASTM D1895
Density 1.38 g/cc0.0499 lb/in³ASTM D792
Water Absorption 0.50 %0.50 %ASTM D570
Linear Mold Shrinkage 0.0112 cm/cm0.0112 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 8686ASTM D785
Tensile Strength, Ultimate 57.0 MPa8270 psiASTM D638
Elongation at Break 0.84 %0.84 %ASTM D638
Tensile Modulus 8.50 GPa1230 ksiASTM D638
Flexural Strength 72.0 MPa10400 psiASTM D790
Flexural Modulus 6.70 GPa972 ksiASTM D790
Compressive Strength 216 MPa31300 psiASTM D695
Izod Impact, Notched 0.251 J/cm0.470 ft-lb/inASTM D256
Charpy Impact, Notched 0.197 J/cm²0.938 ft-lb/in²ASTM D256
Impact 132132J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.70e+14 ohm-cm1.70e+14 ohm-cmASTM D247
Dielectric Constant 4.54.5ASTM D150
Dielectric Strength 10.9 kV/mm277 kV/inShort Time; ASTM D149
Dissipation Factor 0.0480.048ASTM D150
Arc Resistance 77 sec77 secASTM D495
Comparative Tracking Index 175 V175 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 192 °C378 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 153 °C307 °FASTM D648
Shrinkage 0.39 %0.39 %72 hr, 120ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plenco 1581 Polyester, Pellet, Injection Molded
Sumitomo Bakelite Durez® 32633 Glass Filled Phenolic, Injection Grade
Plenco 2311 Phenolic, Granular, Injection Molded

PLEM23m / 50703

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.