MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 905 Polysulfone (PSU), Glass Fiber - UL94
Categories: Polymer; Thermoplastic; Polysulfone (PSU); Polysulfone, 30% Glass Fiber Reinforced

Material Notes: Glass reinforced polysulfone is a rigid, tough material which maintains its properties over a wide temperature range. Additional attributes include dimensional stability, self-extinguishing behavior and good processing characteristics.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.46 g/cc1.46 g/ccASTM D 792
Water Absorption 0.20 %
@Time 86400 sec
0.20 %
@Time 24.0 hour
ASTM D 570
Additive Loading 30 %30 %Primary Additive
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
@Thickness 3.20 mm
0.0010 - 0.0030 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 110 MPa16000 psiASTM D 638
Elongation at Break 2.0 - 3.0 %2.0 - 3.0 %ASTM D 638
Tensile Modulus 8.27 GPa1200 ksiASTM D 638
Flexural Strength 162 MPa23500 psiASTM D 790
Flexural Modulus 7.58 GPa1100 ksiASTM D 790
Izod Impact, Notched 0.747 J/cm
@Thickness 3.20 mm
1.40 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 4.54 J/cm
@Thickness 3.20 mm
8.50 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 21.6 µm/m-°C12.0 µin/in-°FE 831
CTE, linear, Transverse to Flow 48.6 µm/m-°C27.0 µin/in-°FE 831
Deflection Temperature at 1.8 MPa (264 psi) 185 °C365 °FASTM D 648
Flammability, UL94  V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
UL 94
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 332 - 371 °C630 - 700 °F
Mold Temperature 93.3 - 149 °C200 - 300 °F
Drying Temperature 135 °C
@Time 14400 sec
275 °F
@Time 4.00 hour
Moisture Content 0.15 %0.15 %
Dew Point -31.7 °C-25.0 °F
Injection Pressure 68.9 - 124 MPa10000 - 18000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 1499 P X 102560 Polyphenylenesulfone (PPSU), PTFE Lubricated
Celanese FORTRON ICE 504L PPS, 40% Specialty
BASF Ultrason® E 2010 PES
RTP Company RTP 707 High Density Polyethylene (HDPE), Glass Fiber

PQZWA2262 / 91058

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.