MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ITW Insulcast® RTVS 27 NA Silicone Potting/Encapsulation Compound
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Encapsulation Grade

Material Notes: Insulcast® solutions are compounds designed for potting and encapsulating. RTVS 27 NA is a low viscosity, general purpose, reversion resistant RTV Silicone Compound. RTVS 27 NA finds use in commercial potting/casting applications. RTVS 27 NA’s one-to-one ratio by weight or volume makes it ideal for dispensing equipment or hand mixing. With the ability to cure rapidly at elevated temperatures, RTVS 27 NA can be processed quickly in production situations.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.47 g/cc1.47 g/ccUncured. Part A
 1.47 g/cc1.47 g/ccUncured. Part B
Viscosity 2500 cP2500 cPPart A; ASTM D1084
 2700 cP2700 cPMixed, Part A, Part B; ASTM D1084
 3000 cP3000 cPPart B; ASTM D1084
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060ASTM D2240
Tensile Strength 3.45 MPa500 psiASTM D412
Elongation at Break 135 %135 %ASTM D412
Tear Strength 3.16 kN/m18.0 pliDie B; ASTM D624
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.15
@Frequency 1000 Hz
3.15
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 17.7 kV/mm450 kV/inASTM D149
Dissipation Factor 0.0080
@Frequency 1000 Hz
0.0080
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 220 µm/m-°C122 µin/in-°F
Thermal Conductivity 0.360 W/m-K2.50 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C399 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Shrinkage 0.20 %0.20 %
 
Processing PropertiesMetricEnglishComments
Cure Time  15.0 min
@Temperature 95.0 °C
0.250 hour
@Temperature 203 °F
option
 720 - 960 min
@Temperature 25.0 °C
12.0 - 16.0 hour
@Temperature 77.0 °F
option
Pot Life 60.0 - 90.0 min60.0 - 90.0 minPart A, Part B
Shelf Life 6.00 Month6.00 MonthPart A, Part B
 
Descriptive Properties
ColorBuff (Neutral)part B, uncured
 Dark Graypart A, uncured
Mix Ratio by volume1:1Part A: Part B
Mix Ratio by weight1:1Part A: Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWIN9120 / 239630

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.