MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Petropol Nypol® A2 G33 M3 NTLA014 NR203 MSP Nylon 66, 33% Glass Fiber Reinforced, MoS2 Filled, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber/MoS2 Filled

Material Notes: Polyamide 6.6 reinforced with 33% fiberglass, lubricated with 1.5 to 2% molybdenum disulfide (MOS2). Good set of thermal and mechanical properties. Ideal for injection molding.

Information provided by Petropol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 - 1.38 g/cc0.0488 - 0.0499 lb/in³ASTM D792
Water Absorption 1.3 %
@Time 86400 sec
1.3 %
@Time 24.0 hour
ASTM D570
Maximum Moisture Content 0.0200.020
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm0.0030 - 0.0070 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 125 MPa18100 psiASTM D638
Elongation at Break 4.0 %4.0 %ASTM D638
Flexural Strength 205 MPa29700 psiASTM D790
Flexural Modulus 7.00 GPa1020 ksiASTM D790
Izod Impact, Notched 0.900 J/cm1.69 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
Melting Point 250 - 260 °C482 - 500 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 - 280 °C500 - 536 °FMolding
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 90.0 °C194 °F
Dry Time 3.00 hour3.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPETROPOL074 / 312982

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.