MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

DuPont Mobility and Materials Zytel® (PA612) FG158 NC010 PA612  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Unreinforced

Material Notes: Unreinforced Polyamide 612 Developed for Food Contact Applications

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³DAM; ISO 1183
Melt Density 0.900 g/cc0.0325 lb/in³
Water Absorption 3.0 %
@Thickness 2.00 mm
3.0 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Moisture Absorption 1.30 %
@Thickness 2.00 mm
1.30 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Viscosity Number 120 cm³/g1.20 dl/gDAM; ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.015 cm/cm0.015 in/inDAM; ISO 294-4, 2577
 0.011 cm/cm
@Thickness 3.20 mm
0.011 in/in
@Thickness 0.126 in
DAM
Linear Mold Shrinkage, Transverse 0.015 cm/cm0.015 in/inDAM; ISO 294-4, 2577
 0.011 cm/cm
@Thickness 3.20 mm
0.011 in/in
@Thickness 0.126 in
DAM
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 10810850%RH; ISO 2039-2
 114114DAM; ISO 2039-2
Tensile Strength, Yield 52.0 MPa7540 psi50%RH; ISO 527-1/-2
 62.0 MPa8990 psiDAM; ISO 527-1/-2
Film Elongation at Yield, MD 4.3 %4.3 %DAM; ISO 527-3
Elongation at Break 35 %35 %Nominal; DAM; ISO 527-1/-2
 >= 50 %>= 50 %Nominal; 50%RH; ISO 527-1/-2
Elongation at Yield 4.3 %4.3 %DAM; ISO 527-1/-2
 19 %19 %50%RH; ISO 527-1/-2
Tensile Modulus 1.50 GPa218 ksi50%RH; ISO 527-1/-2
 2.40 GPa348 ksiDAM; ISO 527-1/-2
Poissons Ratio 0.380.38DAM
 0.430.4350%RH
Izod Impact, Notched (ISO)  4.00 kJ/m²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 4.50 kJ/m²
@Temperature -30.0 °C
2.14 ft-lb/in²
@Temperature -22.0 °F
50%RH; ISO 180/1A
 5.00 kJ/m²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 6.00 kJ/m²
@Temperature 23.0 °C
2.86 ft-lb/in²
@Temperature 73.4 °F
50%RH; ISO 180/1A
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DAM; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
50%RH; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
DAM; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
50%RH; ISO 179/1eU
Charpy Impact, Notched  0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
50%RH; ISO 179/1eA
 0.420 J/cm²
@Temperature -30.0 °C
2.00 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 0.420 J/cm²
@Temperature 23.0 °C
2.00 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 0.800 J/cm²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
50%RH; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cm50%RH; IEC 62631-3-1
 >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmDAM; IEC 62631-3-1
Surface Resistance 1.00e+12 ohm1.00e+12 ohm50%RH; IEC 62631-3-2
Dielectric Constant  3.2
@Frequency 1e+6 Hz
3.2
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 3.6
@Frequency 100 Hz
3.6
@Frequency 100 Hz
DAM; IEC 62631-2-1
 4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
100Hz; 50%RH; IEC 62631-2-1
 6.0
@Frequency 100 Hz
6.0
@Frequency 100 Hz
100Hz; 50%RH; IEC 62631-2-1
Dielectric Strength 36.0 kV/mm914 kV/inDAM; IEC 60243-1
 36.0 kV/mm914 kV/in50%RH; IEC 60243-1
Dissipation Factor  0.014
@Frequency 100 Hz
0.014
@Frequency 100 Hz
DAM; IEC 62631-2-1
 0.0165
@Frequency 1e+6 Hz
0.0165
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 0.10
@Frequency 1e+6 Hz
0.10
@Frequency 1e+6 Hz
50%RH; IEC 62631-2-1
 0.15
@Frequency 100 Hz
0.15
@Frequency 100 Hz
50%RH; IEC 62631-2-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 120 µm/m-°C66.7 µin/in-°FDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°C66.7 µin/in-°FDAM; ISO 11359-1/-2
Specific Heat Capacity 2.80 J/g-°C0.669 BTU/lb-°FMelt
Thermal Conductivity 0.190 W/m-K1.32 BTU-in/hr-ft²-°FMelt
Melting Point 218 °C424 °F10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 135 °C275 °FDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C144 °FDAM; ISO 75-1/-2
Vicat Softening Point 180 °C
@Load 5.10 kg
356 °F
@Load 11.2 lb
50°C/h; DAM; ISO 306
Glass Transition Temp, Tg 45.0 °C113 °F10°C/min; 50%RH; ISO 11357-1/-2
 60.0 °C140 °F10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94  HB
@Thickness 0.860 mm
HB
@Thickness 0.0339 in
DAM; IEC 60695-11-10
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
DAM; IEC 60695-11-10
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
<= 3.15 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
Oxygen Index 25 %25 %DAM; ISO 4589-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 °C464 °FOptimum, Extrusion
 235 - 250 °C455 - 482 °FExtrusion
 250 °C482 °FOptimum, Injection
 230 - 290 °C446 - 554 °FInjection
Mold Temperature 50.0 - 90.0 °C122 - 194 °FInjection
Drying Temperature 75.0 - 80.0 °C
@Time 10800 - 14400 sec
167 - 176 °F
@Time 3.00 - 4.00 hour
Extrusion; Dehumidified Dryer
Moisture Content 0.060 - 0.15 %0.060 - 0.15 %
 
Descriptive Properties
Delivery formPellets
Drying Recommendedyes
Emission of organic compounds27 µgC/gVDA 277
FMVSS ClassBISO 3795 (FMVSS 302)
ISO designationISO 16396-PA612,,M1G1N,S12-020
Odor Class4VDA 270
Part Marking Code>PA612<ISO 11469
ProcessingCoatable
 Injection Molding
 Other Extrusion
Resin IdentificationPA612ISO 1043
UL 94 recognitionyes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSX5404m / 254521

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.