MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Arkema Pebax® 5533 SP 01 Polyether Block Amide (PEBA)
Categories: Polymer; Thermoplastic; Polyether Block Amide (PEBA)

Material Notes: Polyether block amide PEBAX® 5533 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ISO 1183
 1.01 g/cc0.0365 lb/in³Cond.; ISO 1183
 0.830 g/cc
@Temperature 260 °C
0.0300 lb/in³
@Temperature 500 °F
Melt
Water Absorption 1.2 %1.2 %Dry; Sim. to ISO 62
Moisture Absorption 0.600 %0.600 %Dry; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.012 cm/cm0.012 in/inDry; ISO 294-4, 2577
 0.014 cm/cm0.014 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 50
@Time 15.0 sec
50
@Time 0.00417 hour
Dry; ISO 7619-1
Tensile Strength at Break 52.0 MPa7540 psiDry; ISO 527-1/-2
Tensile Strength, Yield 12.0 MPa1740 psiDry; ISO 527-1/-2
 12.0 MPa1740 psiCond.; ISO 527-1/-2
Tensile Stress at Strain 10.0 MPa
@Strain 10 %
1450 psi
@Strain 10 %
Dry; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %Dry; ISO 527-1/-2
 >= 50 %>= 50 %Cond.; ISO 527-1/-2
 >= 300 %>= 300 %Dry; ISO 527-1/-2
Elongation at Yield 25 %25 %Dry; ISO 527-1/-2
 25 %25 %Cond.; ISO 527-1/-2
Tensile Modulus 0.165 GPa23.9 ksiCond.; ISO 527-1/-2
 0.170 GPa24.7 ksiDry; ISO 527-1/-2
100% Modulus 14.0 MPa
@Strain 100 %
2030 psi
@Strain 100 %
Dry; ISO 527-1/-2
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Dry; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Cond.; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Cond.; ISO 179/1eU
Charpy Impact, Notched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Dry; ISO 179/1eA
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Cond.; ISO 179/1eA
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry; ISO 179/1eA
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Cond.; ISO 179/1eA
Tear Strength 106 kN/m605 pliDry; ISO 34-1
Abrasion 4747mm³; Dry; ISO 4649
Compression Set 43 %
@Temperature 23.0 °C,
Time 86400 sec
43 %
@Temperature 73.4 °F,
Time 24.0 hour
Dry; ISO 815
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.20e+13 ohm-cm3.20e+13 ohm-cmDry; IEC 60093
Surface Resistance 3.00e+12 ohm3.00e+12 ohmCond.; IEC 60093
Dielectric Constant  5.0
@Frequency 1e+6 Hz
5.0
@Frequency 1e+6 Hz
Dry; IEC 60250
 9.0
@Frequency 100 Hz
9.0
@Frequency 100 Hz
Dry; IEC 60250
Dielectric Strength 38.5 kV/mm978 kV/inDry; IEC 60243-1
Dissipation Factor  0.102
@Frequency 1e+6 Hz
0.102
@Frequency 1e+6 Hz
Dry; IEC 60250
 0.111
@Frequency 100 Hz
0.111
@Frequency 100 Hz
Dry; IEC 60250
Comparative Tracking Index 600 V600 VCond.; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 170 µm/m-°C94.4 µin/in-°FDry; ISO 11359-1/-2
Specific Heat Capacity 2.80 J/g-°C0.669 BTU/lb-°FMelt
Thermal Conductivity 0.180 W/m-K
@Temperature 260 °C
1.25 BTU-in/hr-ft²-°F
@Temperature 500 °F
Melt
Melting Point 159 °C318 °F10°C/min; Dry; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 66.0 °C151 °FDry; ISO 75-1/-2
Vicat Softening Point 142 °C288 °F50°C/h 50N; Dry; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °FInjection Molding; ISO 294
Mold Temperature 60.0 °C140 °FInjection Molding; ISO 10724
Injection Velocity 200 mm/sec7.87 in/secInjection Molding; ISO 294
Hold Pressure 30.0 MPa4350 psiInjection Molding; ISO 294
 
Descriptive Properties
Form as DeliveredPellets
Heat StabilizedYes
Light StabilizedYes
Moisture SensitiveYes
Processing MethodsCasting
 Film Extrusion
 Injection Molding
 Other Extrusion
 Profile Extrusion
 Thermoforming
 Transfer Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Pebax® 5533 SA 01 MED Polyether Block Amide (PEBA)
Arkema Pebax® 7233 SA 01 MED Polyether Block Amide (PEBA)
Arkema Pebax® 3533 SP 01 Polyether Block Amide (PEBA)
Arkema Pebax® 5533 SN 70 BLACK Polyether Block Amide (PEBA) (Dry)
Arkema Pebax® 2533 SA 01 Polyether Block Amide (PEBA)

PARKG718 / 142513

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.