LATI Latene® AG7H2 G/50 PP Homopolymer, 50% Glass Fiber Reinforced, Heat Stabilized
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene with 50% Glass Fiber Filler
Material Notes:
Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Glass fibers.
Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America
Information provided by Lati Industria Termoplastici S.p.A.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.32
g/cc
0.0477
lb/in³
Linear Mold Shrinkage, Flow
0.0025
-
0.0050
cm/cm
0.0025
-
0.0050
in/in
Linear Mold Shrinkage, Transverse
0.0075
-
0.0105
cm/cm
0.0075
-
0.0105
in/in
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
40.0
MPa
@Temperature 90.0 °C
5800
psi
@Temperature 194 °F
65.0
MPa
@Temperature 60.0 °C
9430
psi
@Temperature 140 °F
105
MPa
@Temperature 23.0 °C
15200
psi
@Temperature 73.4 °F
Elongation at Break
2.5 %
@Temperature 23.0 °C
2.5 %
@Temperature 73.4 °F
3.4 %
@Temperature 60.0 °C
3.4 %
@Temperature 140 °F
5.8 %
@Temperature 90.0 °C
5.8 %
@Temperature 194 °F
Elongation at Yield
2.7 %
@Temperature 60.0 °C
2.7 %
@Temperature 140 °F
4.2 %
@Temperature 90.0 °C
4.2 %
@Temperature 194 °F
Tensile Modulus
5.30
GPa
@Temperature 90.0 °C
769
ksi
@Temperature 194 °F
8.20
GPa
@Temperature 60.0 °C
1190
ksi
@Temperature 140 °F
10.0
GPa
@Temperature 23.0 °C
1450
ksi
@Temperature 73.4 °F
Charpy Impact Unnotched
1.80
J/cm²
@Temperature -20.0 °C
8.57
ft-lb/in²
@Temperature -4.00 °F
2.00
J/cm²
@Temperature 23.0 °C
9.52
ft-lb/in²
@Temperature 73.4 °F
Charpy Impact, Notched
0.400
J/cm²
@Temperature -20.0 °C
1.90
ft-lb/in²
@Temperature -4.00 °F
0.500
J/cm²
@Temperature 23.0 °C
2.38
ft-lb/in²
@Temperature 73.4 °F
Thermal Properties
Metric
English
Comments
Maximum Service Temperature, Air
125
°C
257
°F
Deflection Temperature at 0.46 MPa (66 psi)
160
°C
320
°F
Deflection Temperature at 1.8 MPa (264 psi)
140
°C
284
°F
Vicat Softening Point
140
°C
@Load 5.00 kg
284
°F
@Load 11.0 lb
Processing Properties
Metric
English
Comments
Melt Temperature
200
-
240
°C
392
-
464
°F
Mold Temperature
40.0
-
60.0
°C
104
-
140
°F
Drying Temperature
80.0
-
90.0
°C
@Time 10800 sec
176
-
194
°F
@Time 3.00 hour
Descriptive Properties
ISO Shrinkage - Pressure
60 MPa
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PLATH9770 / 177466
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.