MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Celanese Celcon® M25HT High Impact Acetal Copolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Impact Modified

Material Notes: Description: Celcon M25HT is an tough acetal copolymer formulated for very high impact properties. It has a high melt strength for extrusion and blow molding applications, while still being injection moldable.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 39.0 MPa5660 psi50 mm/min; ISO 527-2/1A
Tensile Modulus 1.27 GPa184 ksi1 mm/min; ISO 527-2/1A
Flexural Modulus 1.21 GPa175 ksiISO 178
Izod Impact, Notched (ISO) 15.5 kJ/m²7.38 ft-lb/in²ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C154 °FISO 75-1, -2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 199 °C360 - 390 °F
Mold Temperature 77.0 - 93.0 °C171 - 199 °F
Drying Temperature 82.2 °C180 °F
Dry Time 3 hour3 hour
Injection Pressure 75.8 - 110 MPa11000 - 16000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celcon® M25 POM, Unfilled
Celanese Celcon® M25-01 High Molecular Weight Acetal Copolymer
Celanese Celcon® M25N Acetal Copolymer
Celanese Celcon® LW90-F2 POM, Tribological
Celanese Celcon® LM25 Acetal Copolymer (Capable of being Laser Marked)

PHCW10 / 45951

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.