Data provided by Allvac. Applications: Airframe components, cryogenic vessels, heat exchangers, CPI equipment, condenser tubing, pickling baskets. |
UNS R50400; AMS 4902, 4921, 4942; MIL-T-9046, -81556. ASTM F 67, Titanium Grade 2; ASTM B 265, 337, 338, 348; Allvac, an Allegheny Teledyne Company |