MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Plenco 3303 Phenolic, Granular, Injection Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Mineral/Flock Filled

Material Notes: Plenco 03303 is a renumber of Plaslok 5303. Plenco 03303 is a two-stage, mineral and flock-filled phenolic molding compound offering excellent electrical insulating properties. It can be processed by compression, transfer or injection molding . It is UL recognized under file E40654.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.610 g/cc0.0220 lb/in³ASTM D1895
Density 1.54 g/cc0.0556 lb/in³ASTM D792
Water Absorption 0.32 %0.32 %ASTM D570
Linear Mold Shrinkage 0.0084 cm/cm0.0084 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 8383ASTM D785
Tensile Strength, Ultimate 57.0 MPa8270 psiASTM D638
Elongation at Break 0.77 %0.77 %ASTM D638
Tensile Modulus 9.80 GPa1420 ksiASTM D638
Flexural Strength 82.0 MPa11900 psiASTM D790
Flexural Modulus 8.70 GPa1260 ksiASTM D790
Compressive Strength 182 MPa26400 psiASTM D695
Izod Impact, Notched 0.193 J/cm0.362 ft-lb/inASTM D256
Charpy Impact, Notched 0.183 J/cm²0.871 ft-lb/in²ASTM D256
Impact 114114J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.10e+11 ohm-cm3.10e+11 ohm-cmASTM D247
Dielectric Constant 5.55.5ASTM D150
Dielectric Strength 6.20 kV/mm157 kV/inStep by Step; ASTM D149
 9.40 kV/mm239 kV/inShort Time; ASTM D149
Dissipation Factor 0.0680.068ASTM D150
Arc Resistance 180 sec180 secASTM D495
Comparative Tracking Index 175 V175 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 201 °C394 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 168 °C334 °FASTM D648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Shrinkage 0.34 %0.34 %72 hr, 120ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plenco 1501 Polyester, Briquette, Transfer Molded
Plenco 1510 Polyester, Granular, Transfer Molded
Plenco 1508 Polyester, Briquette, Transfer Molded
Plenco 1508 Polyester, Briquette, Injection Molded
Plenco 1501 Polyester, Pellet, Injection Molded

PLEL53o / 50624

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.