MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LG Chemical LUMILOY GN1006F Injection Molding FR mPPO  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, Molded

Material Notes: Uses include electric/electronic parts.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ASTM D792
Water Absorption 0.3 %
@Time 86400 sec
0.3 %
@Time 24.0 hour
ASTM D570
Melt Flow 5.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
5.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 41.2 MPa
@Thickness 3.20 mm
5970 psi
@Thickness 0.126 in
ASTM D638
Elongation at Break 25 %
@Thickness 3.17 mm
25 %
@Thickness 0.125 in
ASTM D638
Flexural Strength 62.8 MPa
@Thickness 3.20 mm
9110 psi
@Thickness 0.126 in
ASTM D790
Flexural Modulus 2.26 GPa
@Thickness 3.20 mm
327 ksi
@Thickness 0.126 in
ASTM D790
Izod Impact, Notched 1.18 J/cm
@Thickness 3.20 mm
2.20 ft-lb/in
@Thickness 0.126 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C
@Thickness 3.20 mm
171 °F
@Thickness 0.126 in
Unannealed; ASTM D648
Flammability, UL94  V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
 V-2
@Thickness 3.00 mm
V-2
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 210 - 240 °C410 - 464 °F
Middle Barrel Temperature 220 - 250 °C428 - 482 °F
Front Barrel Temperature 220 - 250 °C428 - 482 °F
Nozzle Temperature 210 - 240 °C410 - 464 °F
Mold Temperature 50.0 - 70.0 °C122 - 158 °F
Drying Temperature 55 - 70.0 °C130 - 158 °F
Dry Time 2 - 4 hour2 - 4 hour
Moisture Content >= 0.01 %>= 0.01 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUMILOY GN1306F Injection Molding FR Heat Resistant mPPO
Beijing Chemical Industry KAIFA® M105N MPPO Resin
Beijing Chemical Industry KAIFA® M105 MPPO Resin
Beijing Chemical Industry KAIFA® M104N MPPO Resin
Beijing Chemical Industry KAIFA® M104 MPPO Resin

PLGCHEM257 / 146090

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.