MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Borealis LE6006 Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Wire/Cable Grade

Material Notes: It is a low loss LDPE compound for coaxial cables. LE6006 contains a special type of antioxidant, which does not adversely affect the electrical properties. Applications: bamboo constructed cables, coaxial cables, inner skin of radio frequency cables, and telephone wires. Specifications: ISO 1872-PE, KGHN, 18-D003; ASTM D1248 Type I, Class A, Category 5, Grade E4, E5; EN 50290-2-23; DIN VDE 0207, 2YI3; IEC 61196; and EN 50117.

Information provided by Borealis AG

Key Words: LDPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ISO 1183
ESCR 100% Igepal® >= 96 hour
@Temperature 50.0 °C
>= 96 hour
@Temperature 122 °F
F20; IEC 60811-4-1/B
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 50501s; ISO 868
Tensile Strength at Break 15.0 MPa2180 psi50mm/min; ISO 527
Elongation at Break 600 %600 %50mm/min; ISO 527
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+6 ohm-cm1.00e+6 ohm-cmDC; IEC 60093
Dielectric Constant 2.29
@Frequency 1e+6 Hz
2.29
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength >= 22.0 kV/mm>= 559 kV/inIEC 60243
Dissipation Factor 0.000080
@Frequency 1e+6 Hz
0.000080
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -76.0 °C<= -105 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 100 °C176 - 212 °Fconductor preheating temperature
Melt Temperature 200 - 230 °C392 - 446 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade
Borealis Bormed™ LE6601-PH LDPE for Pharmaceutical Blow Molding
Lubrizol Estane® ZHF 80AT3 Thermoplastic Polyurethane, Flame Retardant
Borealis Borstar® LE8706 Natural Bimodal LLDPE Jacketing Compound for Energy and Communication Cables
Braskem D118 Polypropylene Homopolymer

PBOREA519 / 108778

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.