MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Mitsubishi Chemical Advanced Materials Semitron® CMP XL20 (ASTM Product Data Sheet)
Categories: Polymer; Thermoplastic; Polyamide-imide (PAI)

Material Notes:

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccASTM D792
Water Absorption 0.40 %0.40 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 1.7 %1.7 %ASTM D 570(2)
Outgassing - Total Mass Loss 1.85 %1.85 %ASTM E595
Collected Volatile Condensable Material 0.00 %0.00 %ASTM E-595
 
Chemical PropertiesMetricEnglishComments
Ionic Impurities - Na (Sodium) 3.9 ppm3.9 ppmICP/MS
Ionic Impurities - K (Potassium) 0.50 ppm0.50 ppmICP/MS
Ionic Impurities - Fe (Iron) 1.5 ppm1.5 ppmICP/MS
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 8080ASTM D785
Hardness, Rockwell M 120120ASTM D785
Tensile Strength 138 MPa20000 psiASTM D638
Tensile Strength at 150°C (300°F) 103 MPa15000 psiASTM D638
Tensile Strength at 65°C (150°F) 124 MPa18000 psiASTM D638
Elongation at Break 10 %10 %ASTM D638
Tensile Modulus 3.96 GPa575 ksiASTM D638
Flexural Strength 165 MPa24000 psiASTM D790
Flexural Modulus 4.14 GPa600 ksiASTM D790
Compressive Strength 165 MPa24000 psi10% Def.; ASTM D695
Compressive Modulus 2.76 GPa400 ksiASTM D695
Shear Strength 110 MPa16000 psiASTM D732
Izod Impact, Notched 1.1 J/cm2.0 ft-lb/inASTM D256
Coefficient of Friction, Dynamic 0.350.35dry vs. steel; QTM55007
K (wear) Factor >= 2010 x 10-8 mm³/N-M>= 1000 x 10-10 in³-min/ft-lb-hrQTM 55010
Limiting Pressure Velocity 0.140 MPa-m/sec4000 psi-ft/min4:1 safety factor applied; QTM 55010
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+16 ohm>= 1.00e+16 ohmASTM D257
Dielectric Constant 4.2
@Frequency 1e+6 Hz
4.2
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 23 kV/mm580 kV/inShort Term; ASTM D149
Dissipation Factor 0.026
@Frequency 1e+6 Hz
0.026
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.6 µm/m-°C
@Temperature -40.0 - 150 °C
17.0 µin/in-°F
@Temperature -40.0 - 302 °F
ASTM E831
Thermal Conductivity 0.259 W/m-K1.80 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 260 °C500 °FContinuous
Deflection Temperature at 1.8 MPa (264 psi) 278 °C532 °FASTM D648
Glass Transition Temp, Tg 275 °C527 °FAmorphous; ASTM D3418
Flammability, UL94 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
 
Compliance PropertiesMetricEnglishComments
3A-Dairy NoNo
Canada AG NoNo
FDA NoNo
NSF NoNo
USDA NoNo
USP Class VI NoNo
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) LimitedLimited
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) UnacceptableUnacceptable
Alkalies, Weak LimitedLimited
Chlorinated Solvents AcceptableAcceptable
Conductive / Static Dissipative NoNo
Continuous Sunlight LimitedLimited
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Semitron® ESd 480 PEEK, static dissipative, (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Semitron® ESd 520HR (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Semitron® ESd 420 V (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Semitron® MPR-1000 (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Semitron® CMP LL5 Polyester (ASTM Product Data Sheet)

P1SM34e / 89258

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.