MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Lehmann & Voss LUVOCOM® 20-0665 Polyphthalamide with carbon fiber, PTFE, lubricant modified
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), Carbon Fiber + PTFE Filled

Material Notes: Properties/attributes include: Very strong and stiff parts; low coefficient of thermal expansion. Low influence from moisture and temperature to measures and electrical properties, compared with PA66 Electrically conductive, suitable for continuous discharging of statically-generated electricity. Improved friction and wear behavior. Emergency (dry) running property.

Automotive industry, textile- and office machinery, apparatus- and precision engineering. Typical uses include: Bearings, sleeves, sliding elements, control disks, gear wheels, duty parts in switches.

Processing: During processing the moisture level should not exceed 0.05%, otherwise molecular degradation and surface defects (e.g. smearing) may occur. Processing temperatures above 340°C may very rapidly cause thermal damage and should therefore be avoided. The processing notes provided merely represent a recommendation for general use. Due to the large variety of machines, geometries and volumes of parts, etc., it may be necessary to employ different settings according to the specific application. High-temperature polymers place increased demands on the tool steels employed.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.38 g/cc1.38 g/ccISO 1183
Moisture Absorption <= 0.300 %
@Temperature 23.0 °C,
Time 86400 sec
<= 0.300 %
@Temperature 73.4 °F,
Time 24.0 hour
Linear Mold Shrinkage 0.0010 - 0.0040 cm/cm0.0010 - 0.0040 in/inDIN 16901
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 210 MPa30500 psiISO 527-2
Elongation at Break 2.0 %2.0 %ISO 527-2
Modulus of Elasticity 16.0 GPa2320 ksiISO 527-2
Flexural Strength 295 MPa42800 psiISO 178
Flexural Modulus 14.0 GPa2030 ksiISO 178
Flexural Strain at Break 2.8 %2.8 %Flexural Elongation @ Fmax; ISO 178
Charpy Impact Unnotched  3.80 J/cm²
@Temperature -30.0 °C
18.1 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 4.30 J/cm²
@Temperature 23.0 °C
20.5 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eU
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity <= 1e+05<= 1e+05IEC 60167
Surface Resistance <= 10000 ohm<= 10000 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 µm/m-°C11.1 µin/in-°FDIN 53752
Thermal Conductivity 0.360 W/m-K2.50 BTU-in/hr-ft²-°FDIN 52612
Maximum Service Temperature, Air 165 °C329 °FContinuous; UL 746B
 195 °C383 °FShort Term
Deflection Temperature at 1.8 MPa (264 psi) 270 °C518 °FISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 320 - 330 °C608 - 626 °F
Zone 1 320 - 340 °C608 - 644 °F
Zone 2 320 - 345 °C608 - 653 °F
Zone 3 325 - 350 °C617 - 662 °F
Melt Temperature 330 °C626 °F
Mold Temperature 135 - 160 °C275 - 320 °F
Drying Temperature  80.0 °C
@Time >=57600 sec
176 °F
@Time >=16.0 hour
Dehumidifying dryer
 105 °C
@Time 14400 - 18000 sec
221 °F
@Time 4.00 - 5.00 hour
Vacuum Dryer
Moisture Content <= 0.050 %<= 0.050 %
 
Descriptive Properties
Colornatural color (black)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUU8908 / 193867

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.