Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Celanese VECTRA E130i LCP, 30% Glass Reinforced
Categories:
Polymer
;
Thermoplastic
;
Liquid Crystal Polymer (LCP)
;
Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
Material Notes:
High temperature capability, easiest flow. Suitable where very thin walls are required. Used for broad range of SMT applications, with minimal dimensional change. 30% glass filled.
Information provided by Celanese
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.61
g/cc
0.0582
lb/in³
ISO 1183
Moisture Absorption
0.0300 %
0.0300 %
23°C/50%RH; ISO 62
Linear Mold Shrinkage, Flow
0.0010
cm/cm
0.0010
in/in
ISO 294-4
Linear Mold Shrinkage, Transverse
0.0040
cm/cm
0.0040
in/in
ISO 294-4
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell M
71
71
ISO 2039-2
Tensile Strength at Break
150
MPa
21800
psi
5mm/min; ISO 527-2/1A
Elongation at Break
1.6 %
1.6 %
5mm/min; ISO 527-2/1A
Tensile Modulus
15.0
GPa
2180
ksi
50mm/min; ISO 527-2/1A
Flexural Strength
220
MPa
31900
psi
ISO 178
Flexural Modulus
13.5
GPa
1960
ksi
ISO 178
Flexural Strain at Break
2.2 %
2.2 %
ISO 178
Compressive Strength
93.0
MPa
@Strain 1 %
13500
psi
@Strain 1 %
ISO 604
Compressive Modulus
14.0
GPa
2030
ksi
ISO 604
Izod Impact, Notched (ISO)
20.0
kJ/m²
9.52
ft-lb/in²
ISO 180/1A
31.0
kJ/m²
@Temperature 23.0 °C
14.8
ft-lb/in²
@Temperature 73.4 °F
ISO 180/1U
Charpy Impact Unnotched
4.30
J/cm²
20.5
ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched
2.20
J/cm²
10.5
ft-lb/in²
ISO 179/1eA
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+15
ohm-cm
1.00e+15
ohm-cm
IEC 60093
Surface Resistance
1.00e+14
ohm
1.00e+14
ohm
IEC 60093
Dielectric Constant
3.3
@Frequency 1e+6 Hz
3.3
@Frequency 1e+6 Hz
IEC 60250
4.0
@Frequency 100 Hz
4.0
@Frequency 100 Hz
IEC 60250
4.23
@Frequency 2.05e+9 Hz
4.23
@Frequency 2.05e+9 Hz
Dielectric Strength
32.0
kV/mm
813
kV/in
IEC 60243-1
Dissipation Factor
0.010
@Frequency 100 Hz
0.010
@Frequency 100 Hz
IEC 60250
0.025
@Frequency 1e+6 Hz
0.025
@Frequency 1e+6 Hz
IEC 60250
0.060
@Frequency 2.05e+9 Hz
0.060
@Frequency 2.05e+9 Hz
Arc Resistance
140
sec
140
sec
Internal
Comparative Tracking Index
175
V
175
V
IEC 60112
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
7.00
µm/m-°C
3.89
µin/in-°F
ISO 11359-2
CTE, linear, Transverse to Flow
20.0
µm/m-°C
11.1
µin/in-°F
ISO 11359-2
Melting Point
335
°C
635
°F
10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi)
276
°C
529
°F
ISO 75-1, -2
Deflection Temperature at 8.0 MPa
216
°C
421
°F
ISO 75-1, -2
Vicat Softening Point
195
°C
383
°F
ISO 306
Flammability, UL94
V-0
V-0
Oxygen Index
45 %
45 %
ISO 4589
Processing Properties
Metric
English
Comments
Processing Temperature
80.0
-
120
°C
176
-
248
°F
cavity
335
-
345
°C
635
-
653
°F
hot runner
Feed Temperature
60.0
-
80.0
°C
140
-
176
°F
Zone 1
315
-
325
°C
599
-
617
°F
Zone 2
320
-
330
°C
608
-
626
°F
Zone 3
325
-
335
°C
617
-
635
°F
Zone 4
330
-
340
°C
626
-
644
°F
Die Temperature
335
-
345
°C
635
-
653
°F
Melt Temperature
340
°C
644
°F
ISO 294
335
-
345
°C
635
-
653
°F
Mold Temperature
100
°C
212
°F
ISO 294
Injection Velocity
150
mm/sec
5.91
in/sec
ISO 294
Drying Temperature
150
-
170
°C
302
-
338
°F
Dry Time
4.00
-
6.00
hour
4.00
-
6.00
hour
Moisture Content
<= 0.010 %
<= 0.010 %
Injection Pressure
50.0
-
150
MPa
7250
-
21800
psi
Hold Pressure
69.0
MPa
10000
psi
ISO 294
50.0
-
150
MPa
7250
-
21800
psi
Back Pressure
<=
3.00
MPa
<=
435
psi
Screw Speed
80
rpm
@Diameter 40.0 mm
80
rpm
@Diameter 1.57 in
140
rpm
@Diameter 25.0 mm
140
rpm
@Diameter 0.984 in
200
rpm
@Diameter 16.0 mm
200
rpm
@Diameter 0.630 in
Descriptive Properties
Injection molding
Yes
Injection speed
very fast
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Celanese VECTRA A130 LCP, 30% Glass Reinforced
Covestro Bayblend® FR3010 HF PC/ABS Blend
Celanese FORTRON® 1140 E7 Polyphenylene Sulfide (PPS)
Celanese VECTRA E115i LCP, 15% Glass Reinforced
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
PHCQ499 / 178954
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.