System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Zell-Metall Engineering Plastics Zellamid 1100 MO
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, MoS2 Filled
Material Notes:
Improved sliding and self lubricating properties are achieved by the addition of molybdenum disulphide. UV-radiation resistance is enhanced.
Color: black
Applications: For conveyor screws
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.15
g/cc
0.0415
lb/in³
Moisture Absorption at Equilibrium
2.5 - 3.0 %
2.5 - 3.0 %
50% RH
Water Absorption at Saturation
6.0 - 7.0 %
6.0 - 7.0 %
23°C
Mechanical Properties
Metric
English
Comments
Hardness, Shore D
83 - 85
83 - 85
DIN 53505
Ball Indentation Hardness
165
MPa
23900
psi
DIN 53456
Tensile Strength at Break
90.0
-
92.0
MPa
13100
-
13300
psi
DIN 53455
Elongation at Break
10 - 30 %
10 - 30 %
DIN 53455
Tensile Modulus
4.10
GPa
595
ksi
DIN 53457
0.900
GPa
@Temperature 100 °C
131
ksi
@Temperature 212 °F
DIN 53457
Charpy Impact Unnotched
NB
NB
DIN 53453
Charpy Impact, Notched
2.20
-
2.80
J/cm²
10.5
-
13.3
ft-lb/in²
DIN 53453
Coefficient of Friction
0.050 - 0.10
0.050 - 0.10
to steel, added lubrication
0.30 - 0.35
0.30 - 0.35
to steel, no lubrication; ISO/DTR 7147
Abrasion
91
91
mm³; DIN 53516
Thermal Properties
Metric
English
Comments
CTE, linear
80.0
µm/m-°C
@Temperature 20.0 °C
44.4
µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity
1.67
J/g-°C
0.399
BTU/lb-°F
Thermal Conductivity
0.280
W/m-K
1.94
BTU-in/hr-ft²-°F
DIN 52612
Melting Point
220
°C
428
°F
Maximum Service Temperature, Air
100
-
120
°C
212
-
248
°F
long time operation
120
-
140
°C
248
-
284
°F
medium time operation
160
°C
320
°F
a few hours operation
Minimum Service Temperature, Air
-40.0
°C
-40.0
°F
Flammability, UL94
HB
HB
Descriptive Properties
Time yield limit
up to 5
s1/1000; DIN.53444
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Zell-Metall Engineering Plastics Zellamid 250 (PA6.6)
Zell-Metall Engineering Plastics Zellamid 1115 at 50% RH
Zell-Metall Engineering Plastics Zellamid 1100 OIL
Zell-Metall Engineering Plastics Zellamid 1100 MO at 50% RH
Zell-Metall Engineering Plastics Zellamid 1100
PZELL18 / 72947
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.