MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Envalior Stanyl® TW341-N PA46, Dry, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 46 (PA46); Nylon 46, Unreinforced

Material Notes: Heat Stabilized, Lubricated

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ISO 1183
Moisture Absorption 3.70 %3.70 %Humidity; Sim. ISO 62
Linear Mold Shrinkage, Flow 0.020 cm/cm0.020 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.020 cm/cm0.020 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 100 MPa14500 psiISO 527-1/-2
 30.0 MPa
@Temperature 200 °C
4350 psi
@Temperature 392 °F
ISO 527-1/-2
 35.0 MPa
@Temperature 180 °C
5080 psi
@Temperature 356 °F
ISO 527-1/-2
 40.0 MPa
@Temperature 160 °C
5800 psi
@Temperature 320 °F
ISO 527-1/-2
 50.0 MPa
@Temperature 120 °C
7250 psi
@Temperature 248 °F
ISO 527-1/-2
Elongation at Break 40 %40 %Nominal; ISO 527-1/-2
 >= 50 %
@Temperature 120 °C
>= 50 %
@Temperature 248 °F
Nominal; ISO 527-1/-2
 >= 50 %
@Temperature 160 °C
>= 50 %
@Temperature 320 °F
Nominal; ISO 527-1/-2
 >= 50 %
@Temperature 180 °C
>= 50 %
@Temperature 356 °F
Nominal; ISO 527-1/-2
 >= 50 %
@Temperature 200 °C
>= 50 %
@Temperature 392 °F
Nominal; ISO 527-1/-2
Tensile Modulus 3.30 GPa479 ksiISO 527-1/-2
 0.500 GPa
@Temperature 200 °C
72.5 ksi
@Temperature 392 °F
ISO 527-1/-2
 0.600 GPa
@Temperature 180 °C
87.0 ksi
@Temperature 356 °F
ISO 527-1/-2
 0.650 GPa
@Temperature 160 °C
94.3 ksi
@Temperature 320 °F
ISO 527-1/-2
 0.800 GPa
@Temperature 120 °C
116 ksi
@Temperature 248 °F
ISO 527-1/-2
Flexural Modulus 3.00 GPa435 ksiISO 178
 0.600 GPa
@Temperature 160 °C
87.0 ksi
@Temperature 320 °F
ISO 178
 0.800 GPa
@Temperature 120 °C
116 ksi
@Temperature 248 °F
ISO 178
Izod Impact, Notched (ISO)  4.00 kJ/m²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 10.0 kJ/m²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmIEC 60093
Dielectric Strength 25.0 kV/mm635 kV/inIEC 60243-1
Comparative Tracking Index 400 V400 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 85.0 µm/m-°C47.2 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°C61.1 µin/in-°FISO 11359-1/-2
Melting Point 295 °C563 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 190 °C374 °FISO 72-1/-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Stanyl® TW341 PA46, Dry, Heat Stabilized
Envalior Stanyl® TW341 Nylon 46 (European and Asian Grade) (Dry)
Envalior Stanyl® TW341-B PA46, Conditioned, Heat Stabilized
Envalior Stanyl® TW341-N PA46, Conditioned, Heat Stabilized
Röhm Plexiglas® 8N PMMA Molding Compound

PDSM8268 / 184969

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.