Toyobo ECOVYLOPET® EMC2311 PET Bottle Recycling Grade, 10% Glass Reinforced
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polyethylene Terephthalate (PET)
;
Polyethylene Terephthalate (PET), 10% Glass Reinforced
Material Notes:
Features:
PET Bottle Recycling Grade, 10% Glass Fiber Reinforced, General Purpose
Applications:
Automobile engine head covers
Hot plates
Vending machine parts
Umbrella ribs
Information provided by Toyobo.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.38
g/cc
0.0499
lb/in³
Water Absorption
0.050 %
0.050 %
24 hrs at 23°C
Linear Mold Shrinkage, Flow
0.0040
cm/cm
@Thickness 2.00 mm
0.0040
in/in
@Thickness 0.0787 in
Linear Mold Shrinkage, Transverse
0.0090
cm/cm
0.0090
in/in
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell M
90
90
Tensile Strength at Break
80.0
MPa
11600
psi
Elongation at Break
3.1 %
3.1 %
Modulus of Elasticity
4.20
GPa
609
ksi
Flexural Strength
125
MPa
18100
psi
Izod Impact, Notched
0.700
J/cm
1.31
ft-lb/in
Thermal Properties
Metric
English
Comments
CTE, linear
40.0
µm/m-°C
@Temperature 20.0 °C
22.2
µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi)
235
°C
455
°F
0.455 MPa
Deflection Temperature at 1.8 MPa (264 psi)
205
°C
401
°F
Processing Properties
Metric
English
Comments
Mold Temperature
120
°C
248
°F
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Celanese Rynite® 408 NC010 PET (Extended Tabular Temperature Data)
Eastman Aqua 18696 PET
Eastman 5214A PET
Eastman Aqua 20837 PET
Eastman Aqua PJ002 PET
PTOY661 / 70821
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.